This webinar will discuss the proper procedure for applying metallic thermal spray coatings (TSCs) of aluminum, zinc and their alloys and composites to protect steel from corrosion. Standards, required equipment, application procedures, and in-process quality control checkpoints will be discussed. Participants will be eligible to receive credit from SSPC.
Downloadable File:
(right-click and choose 'Save Target As' to download; all downloads are copyright of their author.)
Presenter:

John Kern
SSPC

John Kern is a technical auditor for SSPC. He has over 40 years experience in the industrial coatings industry and over 30 experience in the corrosion industry. He has experience as a Coatings Chemist Tech for New Jersey Department of Transportation, a Corrosion Chemist for the U.S. Navy, and a Coatings Program Engineer for the U.S. Coast Guard. He is a NACE CIP Level 3 #135, an instructor for multiple training courses for SSPC, and a prior vice chair for National Ship Research Program. He is the president, consultant and chief engineer for Virginia Coatings Inspections and a Consultant at ADA Technologies.

Sponsor:

Thermion, Inc.

Thermion is the worldwide leader in High Production Twin Wire Spray Equipment for TSA. We offer full turn-key arc spray systems for many oil & gas applications such as spools, pipe, valves, vessels, flanges, CUI to name a few. Thermion offers complete service beyond equipment such as parts, service, tech support/training, consumables, spray wires/materials, testing equipment and much more. For your next shut down and quick turn around look to Thermion for complete sales, service and support. Please visit www.thermioninc.com.


Register Now


Tagged categories: Coating Application; Coating failure; Coating Materials; Coating types; Corrosion; Galvanized/thermal spray coatings; North America; PaintSquare; Thermal spray


Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 2/24/2020)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us