Fibers Give New 'Textile Concrete' Appeal

Fibers could be the key to lighter, more durable and more versatile form of reinforced concrete, according to a new report from researchers at the Technical University of Dresden.


‘Textile Concrete’ Offers Support Alternative

Researchers at the Technical University of Dresden are investigating a form of reinforced concrete they claim is lighter, more durable and more versatile than conventional materials.


Getting Schooled on Bridge Building

Students at the University of Miami are getting first-hand knowledge of the science of bridge building and materials performance as they actively participate in the construction of a pedestr...


 
 

Articles (1)


Pull-Off Adhesion Strength Testing of
Lining Systems on Concrete

from JPCL, January 2016 ; by Vaughn O’Dea, Cory Brown and Anthony Dallen, Tnemec Company, Inc.

The authors present the common pull-off adhesion test methods used for concrete subst...


 
 

Video Learning Center (15)


Architectural Coatings: A PaintSquare Video Education Series

A collection of archived webinars focused on architectural coatings.


Concrete: A PaintSquare Video Education Series

A collection of archived webinars focused on concrete coatings and maintenance.


see more video learning center collections
 
 

Standards (1)


Standard Test Method for Tensile Properties of Organic Coatings

issued by ASTM

Tensile properties determined by this method are of value in studying the behavior of coatings ...


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
Strategic Materials Inc.

 
Sauereisen, Inc.

 
SAFE Systems, Inc.

 
Abrasives Inc.

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us