Problem Solving Forum (27)


What abrasive should be used to prepare stainless steel?


How can I determine the cleanliness of stainless steel for painting after blast cleaning?


Can glass abrasives be used for surface preparation of carbon steel in shipyards?


What causes static electricity during abrasive blasting? What risk does it pose, and how can it be controlled?


What causes static electricity during abrasive blasting? What risk does it pose, and how can it be controlled?


How do you remove all traces of an uncured internal coating from a tank when abrasive blasting is not an option?


How does abrasive recycling affect cleaning rates when steel is blast-cleaned in the field?


Which type of abrasive blasting media is suitable for preparing the more “exotic” stainless steels, such as Inconel or Monel?


What causes static electricity during abrasive blasting? What risk does it pose, and how can it be controlled?


What is the function of an air receiver during blasting?


How long after blasting can stainless steel be left before painting? If this time is exceeded, what further surface preparation is required?


What abrasive should be used to prepare stainless steel?


What causes static electricity during abrasive blasting? What risk does it pose, and how can it be controlled?


How can I determine the cleanliness of stainless steel for painting after blast cleaning?


How clean must the compressed-air supply be for blast cleaning, blow down and painting? How is cleanliness of the air determined?


How does abrasive recycling affect cleaning rates when steel is blast-cleaned in the field?


What causes static electricity during abrasive blasting? What risk does it pose, and how can it be controlled?


What advantages/disadvantages have you seen with using recycled glass abrasives vs. traditional abrasives?


How do you remove all traces of an uncured internal coating from a tank when abrasive blasting is not an option?


How long can a blasted surface be left before priming under different temperatures/relative humidity environments?


I’ve heard that the use of the proper blast media is critical for the successful application of thermal spray aluminum and other metallics. What mechanism would lead to the differing performance characteristics of the TSA based on the blast media?


Which type of abrasive blasting media is suitable for preparing the more “exotic” stainless steels, such as Inconel or Monel?


What causes static electricity during abrasive blasting? What risk does it pose, and how can it be controlled?


When blasting cast-iron structural steelwork, what type of defects might be found, and how do you address them?


How long can a blasted surface be left before priming under different temperatures/relative humidity environments?


Some painting specifications call for the use of “Best Effort” in relation to blasting. How does one determine “Best Effort?”


What is the remedial action if a blaster produces too high a surface profile for the required primer thickness?


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
NLB Corporation

 
Classic Protective Coatings

 
Paint BidTracker

 
EDCO - Equipment Development Co. Inc.

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
Modern Safety Techniques

 
Julbert, Inc.

 
Sherwin-Williams

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us