The March issue of the Journal of Protective Coatings & Linings is now available in print and online at paintsquare.com. This issue contains feature articles on rail tank car linings,...
|
|
Managing an industrial facility requires one to wear many hats. Everyone from the company president to the forklift operator regularly highlights areas where repairs or improvements are need...
|
|
German special chemicals company Evonik Industries has developed a new coatings technology designed to deliver glossy exterior coatings that are permeable to water vapor from the inside.
|
|
A Pennsylvania nuclear plant is again reporting a coating defect and corrosion in one of its units, near the site of decayed wood left in the structure.
|
|
Ameron executives knew of coating failures and corrosion damage at the Sable Offshore Energy Project well before the company applied for insurance related to those problems, according to the...
|
|
Shipping container manufacturer Sea Box Inc. has filed suit against the Valspar Corp., accusing the coating maker of supplying defective paint for a $40 million container coating project for...
|
|
SAN ANTONIO—A picture may be worth a thousand words, but one squishy word in a contract could trigger a bill that could break your company.
|
|
StondriMVT, new from Stonhard, is a high-solids epoxy system formulated
to suppress excess moisture in concrete before an overlayment.
|
|
Stonhard has introduced a two-component epoxy system specifically designed to suppress excess moisture in concrete.
|
|