A study published earlier this month reportedly found that the inclusion of proteins such as egg yolk were intentional for the “Old Masters” as they prepared their oil paints.
|
|
At the beginning of the month, the General Administration of Customs of the People's Republic of China issued an order abolishing the “Measures for the Supervision and Administration of the ...
|
|
Researchers from Sorbonne University in France recently looked into why tempera paint—also known as egg tempera—was reigned as a supreme medium among Renaissance artists, such as Leonardo Da...
|
|
The University of Illinois at Chicago announced last month that it would be participating in AnalySwift, LLC’s Academic Partner Program to accelerate development and adoption of new material...
|
|
A new research project for waterborne raw materials is being conducted by the Faculty of Applied Natural Sciences at the Technical University of Cologne in collaboration with Covestro.
|
|
Scientists in Germany say they've developed a new method of predicting a coating formulation's leveling outcome, potentially cutting the time needed to test leveling in the lab.
|
|
Researchers have developed a new automated method that predicts the flow outcome of a paint’s properties, which can save on both development time and cost.
|
|
The latest issue of D+D In Depth, featuring four articles on the D+D Elevation Awards winners, the impacts of color and design, gathering paint samples and dealing with lead paint rem...
|
|
Springfield, Missouri, has seen a profusion of artfully painted poles, and more are on the way, according to KSMU Radio.
|
|