The Effect of Feathering on Coating Performance

from JPCL, June 2019 ; by Patrick Cassidy and Michael Kibler, Elzly Technology Corporation; and Cameron Miller, Paul Slebodnick and James Martin, U.S. Naval Research Laboratory

Feedback from waterfront personnel performing maintenance painting for the U.S. Navy ...


Evaluating Material Loss of Steel Under Protective Coatings in Marine Environments

from JPCL, April 2018 ; by Patrick Cassidy and James A. Ellor, P.E., Elzly Technology Corporation; and John Wegand, James Martin, Paul Slebodnick and James Tagert, U.S. Naval Research Laboratory

Over the past 20 years, the U.S. Navy has implemented the use of advanced ultra-high-...


The Effect of Surface Preparation on Coating Performance

from JPCL, July 2016 ; by Patrick Cassidy, Elzly Technology Corporation and Paul Slebodnick, James Tagert and James Martin, U.S. Naval Research Lab

This article describes a study of the effect of profile type, profile height, the ext...


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
Axxiom Manufacturing

 
PaintSquare

 
CRW

 
KTA-Tator, Inc. - Corporate Office

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us