Standards (2)


Standard Terminology and Acronyms Relating to Corrosion

issued by ASTM

1.1 This terminology and acronyms standard covers and defines commonly used terms and acronyms ...


Standard Test Method for Cathodic Disbonding of Pipeline Coatings Subjected to Elevated Temperatures

issued by ASTM

Damage to pipe coating is almost unavoidable during transportation and construction. Breaks or ...


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
Sherwin-Williams

 
base painters

 
Modern Safety Techniques

 
NLB Corporation

 
Thomas Industrial Coatings, Inc.

 
Norton Sandblasting Equipment

 
Paint BidTracker

 
Opta Waterdown, Inc.

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us