Estimating Color Fade of PVDF-Based Topcoats: For ‘Bright Color’ Architectural Restoration and Protective Coating Applications

from D+D In Depth, July 2017 ; by KURT WOOD, ARKEMA INC.

Although many topcoat standards for architectural and protective coating applications...


Coatings for ACM/MCM Panels: Types, Application and Testing

from D+D In Depth, December 2016 ; by James Moses, ALPOLIC Materials, Mitsubishi Plastics Composites America

Aluminum composite materials (ACM) support an inspiring variety of finishes and color...


Painted Aluminum Failures in South Florida Exposure

from D+D In Depth, October 2016 ; by Kirk R. Shields, Corrosion Probe Inc.

Painted aluminum exterior units are rapidly failing in South Florida — sometimes even...


Specifying Coatings for Architectural Metals

from D+D In Depth, September 2016 ; by Gabriel Morales-Sada, AkzoNobel

Choosing the correct coating system for aluminum or galvanized steel substrates depen...


Liquid vs. Powder: A Comparative Review of Fluoropolymer Coatings

from D+D Print, December 2014 ; by Scott Moffatt, PPG Industries

What does the next generation of powder coatings mean for architectural applications ...


The prospects for powder

from JAC, March/April 2009 ; by Allen Zielnik, Atlas Material Testing Technology LLC

The coatings technology gets points for its 'green' profile and resistance properties...


Proving their mettle

from JAC, January/February 2009 ; by Jayson L. Helsel, P.E., KTA-Tator Inc.

Advances in technology expand the choices of high-performance finishes for metallic s...


Insurance policies for painted panels

from JAC, October 2005 ; by Joseph Berchenko

Coil-coated steel makes up the lion’s share of the market for metal panels. This arti...


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
WEFTEC Show

 
Sauereisen, Inc.

 
Strategic Materials Inc.

 
SAFE Systems, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Tarps manufacturing, Inc.

 
DeFelsko Corporation

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us