Hubble Bubble Rising

from JPCL, December 2017 ; by Carl Reed, Greenman-Pedersen, Inc. (GPI), and Dr. Mike O’Donoghue and Vijay Datta, MS, International Paint LLC

This article examines the flaws of the current system of establishing and using speci...


Estimating Color Fade of PVDF-Based Topcoats: For ‘Bright Color’ Architectural Restoration and Protective Coating Applications

from D+D In Depth, July 2017 ; by KURT WOOD, ARKEMA INC.

Although many topcoat standards for architectural and protective coating applications...


Understanding Standards: A Primer on Programs and Purpose

from D+D In Depth, February 2017 ; by ALLEN ZIELNIK, ATLAS MATERIAL TESTING TECHNOLOGY LLC

How does a method, material, or practice ultimately become the accepted standard? Thi...


Corrosion: Domesticated and in the Wild

from JPCL, February 2017 ; by Carl W. Reed, GPI Laboratories, Inc., and Kat Coronado, International Paint, LLC

This article examines the four predominant sources of corrosion that occur “in the wi...


Outdoor Testing Never Lies

from D+D Print, October 2014 ; by Allen Zielnik, Atlas Material Testing Technology LLC

Laboratory weather testing of coatings has come a long way, but exposure to the eleme...


Qualifying Coatings for NASA Launch Facilities

from JPCL, The Facility Owner's Perspective 2014 Special Issue; by Dr. Mark R. Kolody, Jerome P. Curran and Dr. Luz Marina Calle, NASA Corrosion Technology Laboratory

This article discusses the test protocol required for coating systems to be included ...


Specifying and Testing Architectural Cast Stone

from D+D Print, July 2014 ; by Todd Nelson, P.E., Wiss, Janney, Elstner Associates Inc.

Specifiers should be aware of the requirements of ASTM C1364, along with its limitati...


Differential scanning calorimetry

from JPCL, June 2014


Test Method Development for Improved Laboratory Accelerated Weathering of High-Performance Coatings

from D+D Print, January/February 2013 ; by Allen Zielnik, Atlas Material Testing Technology LLC

As this article shows, methods for accelerated weather testing for high-performance c...


On scribing test panels

from JPCL, August 2012

For an in-plant, exterior exposure, or accelerated testing program for coatings, shou...


Comparing Test and Field Performance of Thick-Film Elastomeric Polyureas

from JPCL, July 2010 ; by Dudley J. Primeaux II, PCS, CCI, Primeaux Associates, LLC

This article compares earlier accelerated weathering testing for UV stability to real...


New Waterborne Fluoropolymer Resins for Ultra-Weatherable Coatings

from JPCL, December 2009 ; by Winn Darden and Bob Parker, AGC Chemicals Americas; and Naoko Sumi, Isao Kimura, Masakazu Ataku, and Takashige Maekawa, Asahi Glass Co. Ltd.

this article describes solvent-borne and waterborne FEVE resins as well as the potent...


Investigating Corrosion Protection of Offshore Wind Towers, Part 3: Results of the Laboratory Investigations

from JPCL, November 2009 ; by Andreas W. Momber, Ph.D., Muehlhan AG; Peter Plagemann, Ph.D., and Volkmar Stenzel, Ph.D., Fraunhofer Institute for Manufacturing and Applied Materials Research; and Michael Schneider, Ph.D., Fraunhofer Institute for Ceramic Technologies and Systems

In Part 3 of a three-part series, the authors report on corrosive stress on offshore ...


Products

from JPCL, August 2009

Product News: Floor Coating Cures with UV; Accelerated Test Can Mimic 63 Years of UV;...


Durability - The Changing World of Wood

from JAC, May 2008 ; by Allen Zielnik, Atlast Material Testing Technology LLC

The evolution of wood substrates and coatings adds to the complexity of evaluating co...


The war against water

from JAC, March/April 2008 ; by Allen Zielnik, Atlas Material Testing Technology, LLC

An array of water-repellent and waterproofing measures are enlisted in the never-endi...


Durability: Keeping up appearances

from JAC, Feburary/March 2006 ; by Allen Zielnik, Atlas Materials Testing Technology LLC

Color, gloss measurements add science to the art of selecting coatings that will hold...


Durability: UV resistance - Just the tip of the iceberg for testing of coatings durability

from JAC, April 2005 ; by Allen Zielnik

How to measure sunlight resistance and evaluate UV test data


Corrosion and durability testing: changes in the air

from JAC, January 2005 ; by Allen Zielnik

Advances in methods offer greater ‘real-world’ correlation - Congratulations! Your de...


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
Modern Safety Techniques

 
NLB Corporation

 
Paint BidTracker

 
Sherwin-Williams

 
EDCO - Equipment Development Co. Inc.

 
Classic Protective Coatings

 
Sauereisen, Inc.

 
Julbert, Inc.

 
Tarps manufacturing, Inc.

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us