Problem Solving Forum (38)


What are the best suitable corrosion protection strategies to avoid corrosion due to sweating of gas pipelines? What type of coatings can be applied?


How do you protect concrete against microbiologically influenced corrosion?


How do I deal with the small cracks and fractures that occur along the edges and corners of the stone imprints in some of my stamped concrete work?


What is the best way to prevent corrosion of reinforcing bar in concrete?


What types of measures can be taken on or around metal pipes or columns that penetrate concrete or asphalt paving to reduce corrosion at the interface?


If an owner is using thermal spray aluminum on a pipe exterior as corrosion protection under insulation, and there is a holiday in the coating, will corrosion be substantially accelerated at the base carbon steel, being that the steel is now anodic to the aluminum?


What is the best method for protecting cables on suspension bridges from corrosion?


What are the best cycles to use in cyclic accelerated corrosion testing to achieve the highest correlation with atmospheric exposure in a northern, industrial environment?


Should the surfaces of flanges be coated to prevent corrosion? Why or why not?


How can active corrosion be determined on a live pipeline?


What types of measures can be taken on or around metal pipes or columns that penetrate concrete or asphalt paving to reduce corrosion at the interface?


In preparing for coating, what is the best way to treat a steel surface that has been attacked by microbiologically influenced corrosion?


What are the best cycles to use in cyclic accelerated corrosion testing to achieve the highest correlation with atmospheric exposure in a northern, industrial environment?


What types of measures can be taken on or around metal pipes or columns that penetrate concrete or asphalt paving to reduce corrosion at the interface?


What is most effective treatment for steel contaminated with MIC before painting?


How do you protect concrete against microbiologically influenced corrosion?


What is the best method for protecting cables on suspension bridges from corrosion?


What types of measures can be taken on or around metal pipes or columns that penetrate concrete or asphalt paving to reduce corrosion at the interface?


When performing maintenance surveys on structures that require coatings under insulation, how do you inspect the condition of the coatings?


I am the facility manager for a new amusement park that will operate year-round in a hot, humid environment. Some critical structural steel in the heart of the park needs to be protected from corrosion and at the same time to retain very good appearance properties for as long as possible, since maintenance painting is disruptive. What coating system should I select to achieve the longest useful life, given that cost is a secondary consideration, and how long will this system look good while providing corrosion protection?


When we use field splice plate connections on structural steel projects, how do we prevent rust and rust staining at bolt heads and at the splice plate/steel interface?


Should the surfaces of flanges be coated to prevent corrosion? Why or why not?


Structural engineers often prefer mechanically galvanized bolts for accurate tightening while corrosion experts often prefer hot-dip galvanized bolts for superior corrosion protection. How do you resolve this inherent conflict?


How do I minimize corrosion at the splash zone on sheet pile and piping in brackish water?


In preparing for coating, what is the best way to treat a steel surface that has been attacked by microbiologically influenced corrosion (MIC)?


What types of measures can be taken on or around metal pipes or columns that penetrate concrete or asphalt paving to reduce corrosion at the interface?


How can active corrosion be determined on a live pipeline?


What is the best way to prevent corrosion of reinforcing bar in concrete?


I am the facility manager for a new amusement park that will operate year-round in a hot, humid environment. What protective coating system should I select to achieve the longest useful life (cost is a secondary consideration), and what performance can I expect?


When we use field splice plate connections on structural steel projects, how do we prevent rust and rust staining at bolt heads and at the splice plate/steel interface?


I have galvanized steel in direct contact with powder-coated aluminum in an outdoor exposure. The galvanized steel is corroding. What is the best way to remedy the situation?


Should the surfaces of flanges be coated to prevent corrosion? Why or why not?


What’s the best way to prevent corrosion of reinforcing bar in concrete?


What types of measures can be taken on or around metal pipes or columns that penetrate concrete or asphalt paving to reduce corrosion at the interface?


In preparing for coating, what is the best way to treat a steel surface that has been attacked by microbiologically influenced corrosion (MIC)?


How do I minimize corrosion at the splash zone on sheet pile and piping in brackish water?


How can active corrosion be determined on a live pipeline?


What’s the best way to prevent corrosion of reinforcing bar in concrete?


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
Just Like New Overspray Management

 
base painters

 
Seymour Midwest

 
Quikspray, Inc.

 
Tarps manufacturing, Inc.

 
Nationwide Overspray

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us