Standards (2)


Standard Specification for Strength and Protective Coatings on Steel Industrial Chain Link Fence Framework

issued by ASTM

This specification covers the strength and protective coating requirements for industrial steel...


Standard Test Method for Formability of Zinc-Rich Primer/Chromate Complex Coatings on Steel

issued by ASTM

The results of the combined deformation and tape test are related to the ability of the coated ...


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
Sauereisen, Inc.

 
GMA Garnet USA

 
Axxiom Manufacturing

 
KTA-Tator, Inc. - Corporate Office

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us