Hospital Giant Bans Antimicrobial Use

With insufficient evidence that antimicrobial coatings improve the fight against germs and an increasing concern about spreading toxins, a major health care company has decided to ban the pr...


Universities Benefit From PPG Funding

Two universities are getting a boost for research development thanks to investments from coatings giant PPG.


PPG Funds University Research Projects

Coatings giant PPG is investing in engineering and chemistry research at the collegiate level.


Navy Hopes Coating Will Extend Sub Life

The U.S. Navy is trying out a new painting method to keep marine foul off of attack submarines in an effort to extend the vessels’ service expectancy.


Nanocoatings Set for Mega Growth

Good things come in small packages, as the global market for nanotech-based coatings is poised to show, according to a new forecast.


Smart Coatings Market Set to Surge

Forecasters are expecting a “staggering” and sustained across-the-board growth spurt for the global smart coatings industry.


Smart Money is on Smart Coatings

Enlisted by the military, tended by the medical field, and built up by the construction industry, smart coatings have a brilliant future.


 
 
   

**Commercial white papers, product videos, and other sponsored documents posted on this site are paid content from third-party companies; inclusion and posting on this site does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare. By signing in and viewing or downloading this paid content, you agree to make your name and full contact information available to the sponsor of the content.

Advertisements
 
Mitsubishi Gas Chemical America

 
Sidewinder/Persyst Enterprises, Inc.

 
DeFelsko Corporation

 
Safety Lamp of Houston, Inc.

 
SAFE Systems, Inc.

 
Tarps manufacturing, Inc.

 
Fischer Technology Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
ABKaelin, LLC

 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us