In a recent press release, pigment manufacturer The Eckart Group announced a new additive reported to make anti-stick coatings scratch resistant.
|
|
TransCanada, the firm behind the planned Keystone XL oil pipeline from Alberta to Steele City, Nebraska, appears poised to move forward with construction in 2019 after the U.S. State Departm...
|
|
A new nanoparticle coating for plasticating screws from Nordson Corporation (Westlake, OH) is said to offer improved abrasion and corrosion resistance compared to standard high-velocity oxyg...
|
|
A new superhydrophobic protective coating may soon find a wide range of uses, including buildings, airplanes and mobile phones.
|
|
Scientists in Australia have announced a new superhydrophobic protective coating that could one day find uses ranging from preventing ice formation on airplanes and protecting boat hulls fro...
|
|
Two new U.S. Food and Drug Administration-compliant linings have been added to AkzoNobel’s International-brand protective coatings portfolio.
|
|
Anti-corrosion coatings maker Denso North America (Houston) has released its Protal 7900HT high-temperature two-part epoxy pipeline coating in a new 1000-ml cartridge.
|
|
Truck owners are known to take advantage of protective coatings to safeguard the beds of their vehicles against damage from the loads they haul.
|
|
A new polyaspartic coating with antimicrobial properties has been developed specifically for tanks in the food and beverage industry.
|
|
Scientists at the University of Reading have come up with technology that could eventually be developed into self-healing coatings for buildings as well as other applications.
|
|
Scientists at the University of Reading are at work on a self-healing polymer that may find use in automotive coatings, as well as other industrial and biomedical applications.
|
|
Liquid and powder coatings manufacturer Axalta Coating Systems has announced the global launch of its Alesta Anti-Graffiti powder coatings product line, following what the company describes ...
|
|
Michelman has announced the availability of a new product in its ProHere line of water-based polymer dispersions and emulsions developed for use in metal coatings.
|
|
The unique challenges of coatings for the oil and gas industry is the focus of the next free webinar from JPCL and SSPC.
|
|
A corrosion- and abrasion-resistant coating secured one fledgling Norwegian coatings company the top spot in a competition recognizing the best entrepreneurs from across a range of technolog...
|
|
Chemical manufacturing giant BASF has announced the release of a new polyol that is designed to increase the resistance of indoor flooring in demanding environments, such as industrial wareh...
|
|
A joint venture between industry and academia will work to find solutions for challenges such as corrosion, oxidation and abrasion.
|
|
Finding ways to help coatings address challenges such as corrosion, oxidation and abrasion are a just a few of the solutions that will be under the microscope, so to speak, at a new Pennsylv...
|
|
A new abrasion-resistant overcoating from 3M boasts improved flexibility and is designed to protect the primary corrosion coating on pipelines.
|
|
Chinese material scientists have reportedly developed a new coating so resistant to wear that it keeps knives sharp 100 times longer than current models.
|
|
Tnemec Company has added a new chemical-resistant epoxy coating to its Tank Armor line.
|
|
Sherwin-Williams has introduced a high-build, one-coat polyaspartic urethane designed to accelerate return to service on bridges and other infrastructure projects.
|
|
NEI Corp. has launched a hydrophobic coating designed specifically for metal surfaces in several industrial applications.
|
|
3M Scotchkote has introduced Abrasion Resistant Epoxy Coating (AREC) 328, a 100% solids, two-part epoxy system designed for directional drilling, rocky terrain, and other rugged applications...
|
|