from JPCL, November 2016 ; by David A. Hunter, Hunter Engineering Consulting, Inc.
The author describes the background and basics of composite fiber-reinforced polymer ...
|
|
from JPCL, August 2016 ; by [adapted by] Jim Molnar, UTLX, from the 2015 Mechanical Association Railway Technical Services Annual Conference, Protective Coatings Committee Session
Each year the Mechanical Association of Railcar Technical Services Protective Coating...
|
|
from JPCL, July 2015 ; by Xu Huanhui, CYG Changyuan New Materials Company, Shenzhen, China
The author explains how coupled with the appropriate application and quality control ...
|
|
from D+D Print, September 2014
Whether you're coating walls or stripping them, building new or restoring the histori...
|
|
from D+D Print, May 2014 ; by Gary Henry
Sometimes just getting the surface ready for coating is the hardest part of the job.
|
|
from D+D Print, December 2013 ; by Fred Goodwin, FICRI, FACI, and Frank Apicella, BASF Construction Chemicals
Fast-drying concrete mixtures and construction practices can help slash downtime and ...
|
|
from D+D Print, September/October 2013
From air/vapor barriers to wood coatings, stains and finishes, you’ll find a comprehe...
|
|
from D+D Online Features, D+D February 2013 2013 ; by Tom Stuewe
Preventive maintenance (PM) that makes a good roof better is far more cost-effective ...
|
|
from JPCL, March 2012 ; by Roy Nedal, Marine Service International AS
The author gives a contractor’s view of the present state of ship coating maintenance...
|
|
from PWC, September/October 2010 ; by Marco Caporaso
Preservation is the goal. Know the process, and choose the right materials.
|
|
from JPCL, July 2009
|
|
|
|
**Commercial white papers, product videos, and other sponsored documents posted on this site are
paid content from third-party companies; inclusion and posting on this site
does not imply an endorsement nor recommendation of the content by Technology Publishing/PaintSquare.
By signing in and viewing or downloading this paid content, you agree to make your name and full contact
information available to the sponsor of the content.
|
|
|
Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233
TEL 1-412-431-8300 • FAX 1-412-431-5428 • EMAIL webmaster@paintsquare.com
|
The Technology Publishing Network
|
|
|
|
|