22 recommended systems for All Industries; All Exposures; All Substrates

Tradename
83953 Armourshield
System
Epoxy/Urethane (color)/Urethane (clear)
VOC Range
251-340 g/L
Industry
Specialty Functions
Exposure
Anti-Graffiti
Substrate
Steel
 
Tradename
Armourshield
System
Epoxy (1-2 coats)/Urethane
VOC Range
<100 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Marine Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works
Exposure
Above Ground Pipe Exteriors; Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV; Chemical, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe; Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete; Steel
 
Tradename
Armourshield
System
Epoxy (1-2 coats)/Urethane
VOC Range
251-340 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Marine Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works
Exposure
Above Ground Pipe Exteriors; Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV; Chemical, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe; Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete; Steel
 
Tradename
Armourshield
System
Organic Zinc/Epoxy/Urethane
VOC Range
251-340 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Marine Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works
Exposure
Above Ground Pipe Exteriors; Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV; Chemical, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe; Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete; Steel
 
Tradename
ClovaGuard
System
Epoxy/Epoxy/Epoxy
VOC Range
251-340 g/L
Industry
Marine Industry
Exposure
Interior Mild
Substrate
Steel
 
Tradename
ClovaGuard/Armourshield
System
Epoxy (1-2 coats)/Urethane
VOC Range
251-340 g/L
Industry
Marine Industry
Exposure
Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]
Substrate
Steel
 
Tradename
ClovaLine
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Marine Industry; Power Plants; Pulp & Paper; Specialty Functions; Wastewater Treatment Plants, Municipal
Exposure
Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion - Tertiary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
ClovaLine
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Marine Industry; Power Plants; Pulp & Paper; Specialty Functions; Wastewater Treatment Plants, Municipal
Exposure
Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion - Tertiary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
ClovaLine
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
101-250 g/L
Industry
Chemical & Petrochemical Plants; Marine Industry; Power Plants; Pulp & Paper; Specialty Functions; Wastewater Treatment Plants, Municipal
Exposure
Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion - Tertiary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
Clovaline
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Marine Industry; Power Plants; Pulp & Paper; Specialty Functions; Wastewater Treatment Plants, Municipal
Exposure
Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion - Tertiary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
Clovaline
System
Novolac Epoxy/Novolac Epoxy
VOC Range
251-340 g/L
Industry
Chemical & Petrochemical Plants; Marine Industry; Power Plants; Pulp & Paper; Specialty Functions; Wastewater Treatment Plants, Municipal
Exposure
Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion - Tertiary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
Clovaline girth weld
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Transmission Pipeline
Exposure
Field Joint Coating of Buried Pipe
Substrate
Steel
 
Tradename
ClovaLine Series
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Process Water, Brine, Waste Water]
Substrate
Steel
 
Tradename
Clovamastic
System
Epoxy/Epoxy
VOC Range
101-250 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Marine Industry; Pulp & Paper; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works
Exposure
Ballast Tank Linings; Below Water Line; External of Buried Pipe; Immersion Exposure - Non-Potable Water; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas
Substrate
Concrete; Concrete Floors; Concrete Walls, Ceilings; Steel
 
Tradename
Clovamastic
System
Epoxy/Epoxy/Epoxy
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Marine Industry; Pulp & Paper; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works
Exposure
Ballast Tank Linings; Below Water Line; External of Buried Pipe; Immersion Exposure - Non-Potable Water; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas
Substrate
Concrete; Concrete Floors; Concrete Walls, Ceilings; Steel
 
Tradename
Clovamastic/Armourshield
System
Epoxy (1-2 coats)/Urethane
VOC Range
251-340 g/L
Industry
Bridges; Wastewater Treatment Plants, Municipal
Exposure
Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe; Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete
 
Tradename
Clovatherm
System
IOZinc Rich Primer/Silicone Modified
VOC Range
251-340 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 451 F to 800 F (234 C to 427 C)]
Substrate
Steel
 
Tradename
Clovazinc
System
IOZinc Rich Primer/Silicone Modified
VOC Range
>450 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 801 F to 1200 F (428 C to 649 C)]
Substrate
Steel
 
Tradename
Cloverdale Floor Coatings
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants
Exposure
Interior Process Areas
Substrate
Concrete Floors
 
Tradename
LifeLast
System
Urethane Elastomeric (1 Coat)
VOC Range
<100 g/L
Industry
Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; External of Buried Pipe; Field Joint Coating of Buried Pipe; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Immersion Exposure - Potable Water Approved; Immersion Exposure - Seawater; Interior Exposure Environment; Internal of Buried Pipe
Substrate
Concrete; Steel
 
Tradename
rustex
System
Alkyd (fast dry)
VOC Range
251-340 g/L
Industry
Specialty Functions
Exposure
Shop Primers for Steel
Substrate
 
Tradename
silicone alkyd
System
Alkyd Modified/Alkyd Modified
VOC Range
251-340 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C)]
Substrate
Steel