Company Details
Axalta Coating Systems
|
9800 Genard Rd. |
Houston TX 77041 USA
|
Contact for sales inquiries:
Customer Service
|
Phone number for sales inquiries: 800-247-3886 |
Fax number for sales inquiries: 713-939-4027 |
12 recommended systems for All Industries; All Exposures; All Substrates
Tradename
Alesta
System
Epoxy (1-2 coats)/Fluoropolymer
VOC Range
Industry
Chemical & Petrochemical Plants; Water Works
Exposure
Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Steel
Tradename
Alesta
System
Epoxy/Polyester/Polyester
VOC Range
Industry
Chemical & Petrochemical Plants; Water Works
Exposure
Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Steel
Tradename
Alesta Hi Temp
System
Silicone Modified/Silicone Modified
VOC Range
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]
Substrate
Steel
Tradename
Alesta- Hi Temp
System
Silicone Modified/Silicone Modified
VOC Range
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Dry Heat Resistance from 451 F to 800 F (234 C to 427 C); Dry Heat Resistance from 801 F to 1200 F (428 C to 649 C)]
Substrate
Steel
Tradename
Alesta- Spotless
System
Epoxy/Urethane (color)/Urethane (clear)
VOC Range
Industry
Specialty Functions
Exposure
Anti-Graffiti
Substrate
Steel
Tradename
Corroless- Pipe in Pipe
System
Polyurea Hybrid (1, 2, or 3 coats)
VOC Range
Industry
Wastewater Treatment Plants, Municipal
Exposure
Exterior Weathering, UV, and Mild Chemical
Substrate
Steel
Tradename
Ganicin EE 198
System
Epoxy Zinc-rich/MCU/MCU
VOC Range
Industry
Railcar Industry
Exposure
Exterior Weathering, UV, General Industrial
Substrate
Steel Rail Cars
Tradename
NAP-GARD
System
Fusion-Bonded Epoxy (1-2 coats)
VOC Range
Industry
Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works
Exposure
External of Buried Pipe; Field Joint Coating of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Potable Water Approved; Interior Exposure Environment; Internal of Buried Pipe
Substrate
Steel
Tradename
Nap-Gard or Alesta
System
Fusion-Bonded Epoxy (1-2 coats)
VOC Range
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali; Process Water, Brine, Waste Water]
Substrate
Steel
Tradename
Plascoat PPA 571
System
Polyester/Polyester/Polyester
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe
Substrate
Steel
Tradename
Tufcote EG 189
System
Epoxy/Epoxy/Epoxy
VOC Range
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Alkalis
Tradename
Tufcote EG 198
System
Epoxy/Epoxy
VOC Range
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Hydrocarbons