34 recommended systems for All Industries; All Exposures; All Substrates
Tradename
1000 CS
System
Epoxy Surfacer (two-part)
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Concrete Surfacing Materials
Substrate
Tradename
1200 CS ESD
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants
Exposure
Interior Process Areas
Substrate
Concrete Floors
Tradename
1550 HT
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Power Plants; Specialty Functions
Exposure
FGD Interiors; Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]
Substrate
Steel
Tradename
1550 HT
System
Novolac Epoxy/Novolac Epoxy
VOC Range
<100 g/L
Industry
Power Plants; Specialty Functions
Exposure
FGD Interiors; Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]
Substrate
Steel
Tradename
2300 LS
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Wastewater Treatment Plants, Municipal
Exposure
Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Interior Exposure Environment
Substrate
Concrete; Steel
Tradename
2900 LS
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Power Plants
Exposure
FGD Stack Interiors
Substrate
Steel
Tradename
3300 FS/1000 CS
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Interior Dry Exposure; Interior Severe Wet End Exposure - Paper Machines
Substrate
Concrete Floors; Steel
Tradename
3800 FS
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Interior Exposure Environment; Interior Normal Wet Exposure
Substrate
Concrete; Concrete Floors
Tradename
Fibercoat CR
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Process Water, Brine, Waste Water]
Substrate
Steel
Tradename
Fibercoat/PM-500
System
Epoxy/MCU/MCU
VOC Range
251-340 g/L
Industry
Marine Industry
Exposure
Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]
Substrate
Steel
Tradename
ICO Glaze
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Waterfont, Lock, and Dam Industry
Exposure
Immersion Exposure - Seawater; Interior Process Areas
Substrate
Concrete; Concrete Walls, Ceilings; Steel
Tradename
ICO Glaze
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Waterfont, Lock, and Dam Industry
Exposure
Immersion Exposure - Seawater; Interior Process Areas
Substrate
Concrete; Concrete Walls, Ceilings; Steel
Tradename
ICO Hi Guard
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Power Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Chemical Exposure - Acid; Chemical Exposure - Caustic; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Secondary Containment
Substrate
Concrete
Tradename
ICO Hi Guard Coating
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Chemical/Water Exposure - Caustic or Acid
Substrate
Concrete
Tradename
ICO Primer LV/Fibercoat
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Water Works; Waterfont, Lock, and Dam Industry
Exposure
Immersion Exposure - Non-Potable Water; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Concrete
Tradename
ICO Primer LV/PM-500
System
Epoxy/MCU/MCU
VOC Range
251-340 g/L
Industry
Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Exterior Exposure - Weathering and UV; Exterior Weathering, UV, and Mild Chemical; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt
Substrate
Concrete
Tradename
ICO Primer LV/PM-500
System
Epoxy/Polyester/Polyester
VOC Range
251-340 g/L
Industry
Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Exterior Exposure - Weathering and UV; Exterior Weathering, UV, and Mild Chemical; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt
Substrate
Concrete
Tradename
ICO Primer XT/Fibercoat
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Waterfont, Lock, and Dam Industry
Exposure
Immersion Exposure - Freshwater
Substrate
Concrete
Tradename
ICO Rust Guard
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil]
Substrate
Steel
Tradename
ICO Rust Guard/Fibercoat
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Pulp & Paper; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Interior Normal Wet Exposure; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Steel
Tradename
ICO Rust Guard/Fibercoat CR
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Chemical Exposure - Acid; Chemical Exposure - Caustic
Substrate
Steel
Tradename
ICO Rust Guard/Fibercoat CR
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Chemical Exposure - Acid; Chemical Exposure - Caustic
Substrate
Steel
Tradename
ICO Rust Guard/Fibercoiat
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Interior Dry Exposure
Substrate
Steel
Tradename
ICO Rust Guard/ICO Glaze
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Marine Industry
Exposure
Interior Mild
Substrate
Steel
Tradename
ICO Rust Guard/PM-500
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
251-340 g/L
Industry
Marine Industry; Power Plants; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Chemical/Water Exposure - Caustic or Acid; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt
Substrate
Steel
Tradename
ICO Rust Guard/PM-500
System
Epoxy/MCU/MCU
VOC Range
251-340 g/L
Industry
Marine Industry; Power Plants; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Chemical/Water Exposure - Caustic or Acid; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt
Substrate
Steel
Tradename
ICO Rust Guard/PM-500
System
Epoxy/Polyester/Polyester
VOC Range
251-340 g/L
Industry
Marine Industry; Power Plants; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Chemical/Water Exposure - Caustic or Acid; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt
Substrate
Steel
Tradename
ICO Rust Guard/PM-500
System
Urethane/Urethane
VOC Range
251-340 g/L
Industry
Marine Industry; Power Plants; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Chemical/Water Exposure - Caustic or Acid; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt
Substrate
Steel
Tradename
ICO Rust Guartd/Fibercoat CR
System
Epoxy/Epoxy/Epoxy
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Chemical/Water Exposure - Wet Fly Ash
Substrate
Steel
Tradename
Milamar 2600 LS
System
Epoxy/Epoxy/Epoxy
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Chemical/Water Exposure - Wet Fly Ash
Substrate
Concrete
Tradename
Milamar 6800 LS
System
Vinyl Ester/Vinyl Ester/Vinyl Ester
VOC Range
101-250 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Acid, Oxidizer, Alkali]
Substrate
Steel
Tradename
Milamar 6850 CS
System
Vinyl Ester/Vinyl Ester/Vinyl Ester
VOC Range
101-250 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Steel
Tradename
PolyMax 250V
System
Epoxy (1-2 coats)/Urethane
VOC Range
101-250 g/L
Industry
Pulp & Paper
Exposure
Interior Dry Exposure
Substrate
Concrete Walls, Ceilings
Tradename
PolyMax 250V-550
System
Epoxy (1-2 coats)/Urethane
VOC Range
101-250 g/L
Industry
Wastewater Treatment Plants, Municipal
Exposure
Interior Exposure Environment
Substrate
Concrete Walls, Ceilings