Duromar, Inc.
706 Washington Street
Pembroke MA 02359 USA

Contact for sales inquiries: Daniel Toft
Phone number for sales inquiries: 781-826-2525
Fax number for sales inquiries: 781-826-2150

 

48 recommended systems for All Industries; All Exposures; All Substrates

Tradename
HPL-1511 + HPL-6700
System
Organic Zinc/Epoxy/Siloxane
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Severe
Substrate
Steel
 
Tradename
1011-Series
System
Inorganic Zinc
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Shop Primers for Steel
Substrate
 
Tradename
DF-1301 + DF-4301
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Secondary Containment
Substrate
Concrete
 
Tradename
DF-1301 + HPL-4301
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Concrete
 
Tradename
DF-1301 + HPL-6210
System
Epoxy/Epoxy
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate
Substrate
Concrete
 
Tradename
DF-1301 + HPL-6210 + HPL-6210
System
Epoxy/Epoxy/Epoxy
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Severe
Substrate
Concrete
 
Tradename
DF-1302 / DF-4301
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Chemical Exposure - Acid; Secondary Containment
Substrate
Concrete
 
Tradename
GMC-Putty / RP-C
System
Other Special Block Filler
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Concrete Surfacing Materials
Substrate
 
Tradename
Happy Hoves - PUA
System
Polyurea Pure (1, 2, or 3 coats)
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Livestock Carriers
 
Tradename
HPL-1011 WB-IOZ
System
Inorganic Zinc-Rich
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 451 F to 800 F (234 C to 427 C)]
Substrate
Steel
 
Tradename
HPL-1011WBZn + HPL-1511 + HPL-6700
System
Organic Zinc/Epoxy/Siloxane
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate
Substrate
Steel
 
Tradename
HPL-1011WBZn + HPL-5611
System
Organic Zinc/Polyurea Hybrid
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Exterior Weathering, UV, General Industrial
Substrate
Steel Locomotive; Steel Rail Cars
 
Tradename
HPL-1110 / HPL-1110
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Marine Industry; Offshore Industry; Pulp & Paper; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Cargo Hold Linings; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Interior Dry Exposure; Interior Exposure Environment; Interior Mild; Interior Normal Wet Exposure; Interior Severe Wet End Exposure - Paper Machines; Jacket [Atmospheric Zone]; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Concrete; Concrete Walls, Ceilings; Steel
 
Tradename
HPL-1110 / HPL-6210
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Transmission Pipeline
Exposure
Above Ground Pipe Exteriors
Substrate
Concrete; Steel
 
Tradename
HPL-1110 PW / HPL-1110-PW
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Water Works
Exposure
Immersion Exposure - Potable Water Approved
Substrate
Steel
 
Tradename
HPL-1110-PW / HPL-1110-PW
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Water Works
Exposure
Immersion Exposure - Potable Water Approved
Substrate
Concrete
 
Tradename
HPL-1301 / DF-4301
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Secondary Containment
Substrate
Concrete
 
Tradename
HPL-1301 + HPL-4310FDA
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants
Exposure
Interior Process Areas
Substrate
Concrete Floors
 
Tradename
HPL-1301, DF-1310
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Interior Normal Wet Exposure; Interior Severe Wet End Exposure - Paper Machines
Substrate
Concrete; Concrete Floors
 
Tradename
HPL-1301, DF-4301
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Power Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Chemical Exposure - Caustic; Chemical/Water Exposure - Wet Fly Ash; Immersion - Tertiary Treatment; Secondary Containment
Substrate
Concrete
 
Tradename
HPL-1301,DF-4301
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Chemical/Water Exposure - Caustic or Acid
Substrate
Concrete
 
Tradename
HPL-1511 + HPL-6210
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Steel
 
Tradename
HPL-2131
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Power Plants
Exposure
FGD Interiors
Substrate
Steel
 
Tradename
HPL-2221
System
Epoxy Phenolic/Epoxy Phenolic
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]
Substrate
Steel
 
Tradename
HPL-2221 / HPL-2221
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Bulk Solids
 
Tradename
HPL-2221-UV / HPL-2221-UV
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Marine Industry
Exposure
Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]
Substrate
Steel
 
Tradename
HPL-2310
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Alkalis
 
Tradename
HPL-2310 / HPL-2310
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Hydrocarbons
 
Tradename
HPL-2310 or HPL-3320 or HPL-3721
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil]
Substrate
Steel
 
Tradename
HPL-2510 / HPL-2510
System
Epoxy (1-2 coats)/Urethane
VOC Range
<100 g/L
Industry
Marine Industry; Offshore Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Waterfont, Lock, and Dam Industry
Exposure
Cargo Tank Linings; External of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Seawater; Internal of Buried Pipe; Topsides [Severe Marine Exposure]
Substrate
Concrete; Steel
 
Tradename
HPL-2510 / HPL-2510
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Marine Industry; Offshore Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Waterfont, Lock, and Dam Industry
Exposure
Cargo Tank Linings; External of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Seawater; Internal of Buried Pipe; Topsides [Severe Marine Exposure]
Substrate
Concrete; Steel
 
Tradename
HPL-2510 / HPL-2510-FR
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Marine Industry; Offshore Industry; Power Plants
Exposure
Below Water Line; Circulating Water Pipe; Jacket [Immersed Area; Splash Zone]
Substrate
Concrete; Steel
 
Tradename
HPL-2510 FR / HPL-2221 LSE
System
Fouling Release
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Antifoulant and Foulant Release Coatings
Substrate
Concrete; Steel
 
Tradename
HPL-2510 or HPL-4315FG
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Process Water, Brine, Waste Water]
Substrate
Steel
 
Tradename
HPL-2510/ HPL-2510
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Marine Industry
Exposure
Ballast Tank Linings
Substrate
Steel
 
Tradename
HPL-2510FDA
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants
Exposure
Interior Process Areas
Substrate
Concrete Walls, Ceilings
 
Tradename
HPL-2510-N / HPL-2510-N
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Primary Containment (Nuclear Only)
Substrate
 
Tradename
HPL-4000 series
System
Novolac Epoxy/Novolac Epoxy
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C)]
Substrate
Steel
 
Tradename
HPL-4310 /HPL-4310
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Chemical Exposure - Caustic
Substrate
Steel
 
Tradename
HPL-4310 / HPL-4310
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Power Plants; Pulp & Paper
Exposure
Chemical Exposure - Acid; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; FGD Stack Interiors
Substrate
Steel
 
Tradename
HPL-4310 / HPL-4310
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Power Plants; Pulp & Paper
Exposure
Chemical Exposure - Acid; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; FGD Stack Interiors
Substrate
Steel
 
Tradename
HPL-4310 or HPL-4320XC
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Acid, Oxidizer, Alkali]
Substrate
Steel
 
Tradename
HPL-4310FDA-FG
System
Epoxy Flake Filled/Epoxy Flake Filled
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Dairy
 
Tradename
HPL-4320XC
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Acids
 
Tradename
HPL-6700
System
Silicone Modified/Silicone Modified
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 801 F to 1200 F (428 C to 649 C)]
Substrate
Steel
 
Tradename
HydroFlor Sealer, HydroFlor
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Interior Dry Exposure; Interior Exposure Environment
Substrate
Concrete Floors
 
Tradename
LSE-Series
System
Epoxy (1-2 coats)/Fluoropolymer
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Anti-Graffiti
Substrate
Concrete; Steel
 
Tradename
PPX-ARO
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Transmission Pipeline
Exposure
Field Joint Coating of Buried Pipe
Substrate
Concrete; Steel