Company Details
Hempel (USA), Inc.
|
600 Conroe Park North Drive |
Conroe TX 77303 USA
|
Contact for sales inquiries:
Marsha Parker
|
Phone number for sales inquiries: 936-523-6000 |
Fax number for sales inquiries: 936-523-6073 |
34 recommended systems for All Industries; All Exposures; All Substrates
Tradename
AvantGuard Series/Hempadur Series/Hempathane Series
System
Organic Zinc/Epoxy/Urethane
VOC Range
Industry
Chemical & Petrochemical Plants
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Steel
Tradename
AvantGuard Series/Quattro Series/Hempaxane
System
Epoxy/Epoxy/Siloxane
VOC Range
Industry
Offshore Industry
Exposure
Topsides [Severe Marine Exposure]
Substrate
Steel
Tradename
Galvosil Series/Hempel"s Silicone Series
System
IOZinc Rich Primer/Silicone Unmodified
VOC Range
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 451 F to 800 F (234 C to 427 C)]
Substrate
Steel
Tradename
Hempadur and Hempathane Series
System
Epoxy (1-2 coats)/Urethane
VOC Range
Industry
Marine Industry
Exposure
Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]
Substrate
Steel
Tradename
Hempadur Mastic 45883
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
Industry
Railcar Industry
Exposure
Exterior Weathering, UV, General Industrial
Substrate
Steel Rail Cars
Tradename
Hempadur Preprep/Hempadur/Hempathane Series
System
Epoxy (1-2 coats)/Urethane
VOC Range
Industry
Chemical & Petrochemical Plants
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Concrete
Tradename
Hempadur Series
System
Epoxy (1-2 coats)/Urethane
VOC Range
Industry
Marine Industry; Railcar Industry; Specialty Functions; Transmission Pipeline; Water Works
Exposure
Ballast Tank Linings; Cargo Hold Linings; Cargo Tank Linings; External of Buried Pipe; Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion Exposure - Non-Potable Water; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Livestock Carriers; Steel
Tradename
Hempadur Series
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
Industry
Marine Industry; Railcar Industry; Specialty Functions; Transmission Pipeline; Water Works
Exposure
Ballast Tank Linings; Cargo Hold Linings; Cargo Tank Linings; External of Buried Pipe; Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion Exposure - Non-Potable Water; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Livestock Carriers; Steel
Tradename
Hempadur Series
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
Industry
Marine Industry; Railcar Industry; Specialty Functions; Transmission Pipeline; Water Works
Exposure
Ballast Tank Linings; Cargo Hold Linings; Cargo Tank Linings; External of Buried Pipe; Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion Exposure - Non-Potable Water; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Livestock Carriers; Steel
Tradename
Hempadur Series
System
Epoxy Phenolic/Epoxy Phenolic
VOC Range
Industry
Marine Industry; Railcar Industry; Specialty Functions; Transmission Pipeline; Water Works
Exposure
Ballast Tank Linings; Cargo Hold Linings; Cargo Tank Linings; External of Buried Pipe; Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion Exposure - Non-Potable Water; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Livestock Carriers; Steel
Tradename
Hempadur Series
System
Epoxy Phenolic/Epoxy Phenolic/Epoxy Phenolic
VOC Range
Industry
Marine Industry; Railcar Industry; Specialty Functions; Transmission Pipeline; Water Works
Exposure
Ballast Tank Linings; Cargo Hold Linings; Cargo Tank Linings; External of Buried Pipe; Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion Exposure - Non-Potable Water; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Livestock Carriers; Steel
Tradename
Hempadur Series
System
Epoxy/Epoxy
VOC Range
Industry
Marine Industry; Railcar Industry; Specialty Functions; Transmission Pipeline; Water Works
Exposure
Ballast Tank Linings; Cargo Hold Linings; Cargo Tank Linings; External of Buried Pipe; Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion Exposure - Non-Potable Water; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Livestock Carriers; Steel
Tradename
Hempadur Series
System
Epoxy/Epoxy/Epoxy
VOC Range
Industry
Marine Industry; Railcar Industry; Specialty Functions; Transmission Pipeline; Water Works
Exposure
Ballast Tank Linings; Cargo Hold Linings; Cargo Tank Linings; External of Buried Pipe; Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion Exposure - Non-Potable Water; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Livestock Carriers; Steel
Tradename
Hempadur Series
System
Other
VOC Range
Industry
Marine Industry; Railcar Industry; Specialty Functions; Transmission Pipeline; Water Works
Exposure
Ballast Tank Linings; Cargo Hold Linings; Cargo Tank Linings; External of Buried Pipe; Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]; Immersion Exposure - Non-Potable Water; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Livestock Carriers; Steel
Tradename
Hempadur Series and Fouling Control Products
System
Other
VOC Range
Industry
Marine Industry
Exposure
Below Water Line
Substrate
Steel
Tradename
Hempadur Series/Hempathane Series
System
Epoxy (1-2 coats)/Urethane
VOC Range
Industry
Wastewater Treatment Plants, Municipal; Water Works
Exposure
Exterior Exposure - Weathering and UV; Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete; Steel
Tradename
Hempalin Series or Hempadur Series
System
Alkyd/Alkyd/Alkyd
VOC Range
Industry
Marine Industry
Exposure
Interior Mild
Substrate
Steel
Tradename
Hempaline
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Hydrocarbons
Tradename
Hempaline Series
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
Industry
Chemical & Petrochemical Plants; Power Plants; Transmission Pipeline; Wastewater Treatment Plants, Municipal
Exposure
Chemical/Water Exposure - Caustic or Acid; Circulating Water Pipe; External of Buried Pipe; FGD Interiors; FGD Stack Interiors; Field Joint Coating of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali; Process Water, Brine, Waste Water]; Secondary Containment
Substrate
Concrete; Steel
Tradename
Hempaline Series
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
Industry
Chemical & Petrochemical Plants; Power Plants; Transmission Pipeline; Wastewater Treatment Plants, Municipal
Exposure
Chemical/Water Exposure - Caustic or Acid; Circulating Water Pipe; External of Buried Pipe; FGD Interiors; FGD Stack Interiors; Field Joint Coating of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali; Process Water, Brine, Waste Water]; Secondary Containment
Substrate
Concrete; Steel
Tradename
Hempaline Series
System
Epoxy/Epoxy 100% solids
VOC Range
Industry
Chemical & Petrochemical Plants; Power Plants; Transmission Pipeline; Wastewater Treatment Plants, Municipal
Exposure
Chemical/Water Exposure - Caustic or Acid; Circulating Water Pipe; External of Buried Pipe; FGD Interiors; FGD Stack Interiors; Field Joint Coating of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali; Process Water, Brine, Waste Water]; Secondary Containment
Substrate
Concrete; Steel
Tradename
Hempaline Series
System
Inorganic Zinc/Epoxy 100% solids
VOC Range
Industry
Chemical & Petrochemical Plants; Power Plants; Transmission Pipeline; Wastewater Treatment Plants, Municipal
Exposure
Chemical/Water Exposure - Caustic or Acid; Circulating Water Pipe; External of Buried Pipe; FGD Interiors; FGD Stack Interiors; Field Joint Coating of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali; Process Water, Brine, Waste Water]; Secondary Containment
Substrate
Concrete; Steel
Tradename
Hempasil and Hempaguard
System
Fouling Release
VOC Range
Industry
Specialty Functions
Exposure
Antifoulant and Foulant Release Coatings
Substrate
Steel
Tradename
Hempel"s Preprep/Hempadur Series/Hempathane Series
System
Epoxy (1-2 coats)/Urethane
VOC Range
Industry
Water Works
Exposure
Exterior Exposure - Weathering and UV
Substrate
Concrete
Tradename
Hempel"s Shop Primer
System
Inorganic Zinc
VOC Range
Industry
Specialty Functions
Exposure
Shop Primers for Steel
Substrate
Tradename
Hempel"s Silicone Series
System
Silicone Unmodified/Silicone Unmodified
VOC Range
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 801 F to 1200 F (428 C to 649 C)]
Substrate
Steel
Tradename
Neocrete SL
System
Epoxy (1-2 coats)/Urethane
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas; Interior Severe Wet End Exposure - Paper Machines
Substrate
Concrete; Concrete Floors
Tradename
Neocrete SL
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas; Interior Severe Wet End Exposure - Paper Machines
Substrate
Concrete; Concrete Floors
Tradename
Peda-Gard SC
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Secondary Containment
Substrate
Concrete
Tradename
Quattro Series
System
Epoxy/Epoxy/Epoxy
VOC Range
Industry
Offshore Industry
Exposure
Jacket [Immersed Area]
Substrate
Steel
Tradename
Quattro Series/Hempadur Series
System
Epoxy/Epoxy Flake Filled/Epoxy Flake Filled
VOC Range
Industry
Offshore Industry
Exposure
Jacket [Splash Zone]
Substrate
Steel
Tradename
Quattro Series/Hempathane
System
Epoxy (1-2 coats)/Urethane
VOC Range
Industry
Transmission Pipeline
Exposure
Above Ground Pipe Exteriors
Substrate
Steel
Tradename
Quattro Series/Hempathane Series
System
Organic Zinc/Epoxy/Siloxane
VOC Range
Industry
Offshore Industry
Exposure
Jacket [Atmospheric Zone]
Substrate
Steel
Tradename
Wall-Gard HD
System
Epoxy (1-2 coats)/Urethane
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper
Exposure
Interior Dry Exposure; Interior Process Areas
Substrate
Concrete Walls, Ceilings