20 recommended systems for All Industries; All Exposures; All Substrates
Tradename
Corrverter
System
Corrosion Protection
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Conversion Coatings
Substrate
Tradename
VpCI 2026
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Chemical Exposure - Acid; Chemical Exposure - Caustic; Interior Dry Exposure; Interior Exposure Environment; Interior Process Areas; Interior Severe Wet End Exposure - Paper Machines; Secondary Containment
Substrate
Concrete; Concrete Floors
Tradename
VpCI 2026
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Chemical Exposure - Acid; Chemical Exposure - Caustic; Interior Dry Exposure; Interior Exposure Environment; Interior Process Areas; Interior Severe Wet End Exposure - Paper Machines; Secondary Containment
Substrate
Concrete; Concrete Floors
Tradename
VpCI 2026/2026
System
Novolac Epoxy/Novolac Epoxy
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Under Insulation, Wet Heat Resistance up to 300 F (149 C)]
Substrate
Steel
Tradename
VpCI 371
System
Silicone Modified/Silicone Modified
VOC Range
341-450 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Dry Heat Resistance from 451 F to 800 F (234 C to 427 C); Dry Heat Resistance from 801 F to 1200 F (428 C to 649 C)]
Substrate
Steel
Tradename
VpCI 386
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Marine Industry; Pulp & Paper; Wastewater Treatment Plants, Municipal; Water Works
Exposure
Exterior Exposure - Weathering and UV; Interior Dry Exposure; Interior Exposure Environment; Interior Mild
Substrate
Concrete; Concrete Walls, Ceilings; Steel
Tradename
VpCI 390
System
Alkyd (fast dry)
VOC Range
101-250 g/L
Industry
Specialty Functions
Exposure
Shop Primers for Steel
Substrate
Tradename
VpCI 395/2026
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Power Plants; Pulp & Paper; Railcar Industry; Wastewater Treatment Plants, Municipal
Exposure
Chemical Exposure - Acid; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Interior Severe Wet End Exposure - Paper Machines; Linings for Steel Rail Car Interiors; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali; Process Water, Brine, Waste Water]; Secondary Containment
Substrate
Acids; Alkalis; Bulk Solids; Concrete; Dairy; Hydrocarbons; Livestock Carriers; Steel
Tradename
VpCI 395/384
System
Epoxy (1-2 coats)/Urethane
VOC Range
341-450 g/L
Industry
Chemical & Petrochemical Plants; Specialty Functions; Waterfont, Lock, and Dam Industry
Exposure
Anti-Graffiti; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Concrete; Steel
Tradename
VpCI 395/384
System
Epoxy/Urethane (color)/Urethane (clear)
VOC Range
341-450 g/L
Industry
Chemical & Petrochemical Plants; Specialty Functions; Waterfont, Lock, and Dam Industry
Exposure
Anti-Graffiti; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Concrete; Steel
Tradename
VpCI 395/386
System
Epoxy (1-2 coats)/Acrylic (1-2 coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Wastewater Treatment Plants, Municipal
Exposure
Exterior Weathering, UV, and Mild Chemical; Interior Process Areas
Substrate
Concrete; Concrete Walls, Ceilings; Steel
Tradename
VpCI 395/395
System
Epoxy/Epoxy
VOC Range
<100 g/L
Industry
Power Plants; Pulp & Paper; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Circulating Water Pipe; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Immersion Exposure - Potable Water Approved; Immersion Exposure - Seawater; Interior Normal Wet Exposure
Substrate
Concrete; Steel
Tradename
VpCI 396Z/395/395
System
Organic Zinc/Epoxy/Epoxy
VOC Range
341-450 g/L
Industry
Marine Industry; Offshore Industry
Exposure
Ballast Tank Linings; Below Water Line; Cargo Hold Linings; Cargo Tank Linings; Jacket [Immersed Area; Splash Zone]
Substrate
Steel
Tradename
VpCI 396Z/396/384
System
Organic Zinc/Urethane/Urethane
VOC Range
341-450 g/L
Industry
Marine Industry; Offshore Industry; Waterfont, Lock, and Dam Industry
Exposure
Exterior Superstructures [Marine, Weathering, & UV]; Jacket [Atmospheric Zone]; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion; Topsides [Severe Marine Exposure]
Substrate
Steel
Tradename
VpCI-386
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Exterior Weathering, UV, General Industrial
Substrate
Steel Rail Cars
Tradename
VpCI-395/386
System
Epoxy (1-2 coats)/Acrylic (1-2 coats)
VOC Range
<100 g/L
Industry
Transmission Pipeline
Exposure
Above Ground Pipe Exteriors
Substrate
Concrete; Steel
Tradename
VpCI-395/395
System
Epoxy/Epoxy
VOC Range
<100 g/L
Industry
Transmission Pipeline
Exposure
External of Buried Pipe; Field Joint Coating of Buried Pipe; Internal of Buried Pipe
Substrate
Concrete; Steel
Tradename
VpCI-396/384
System
Urethane/Urethane
VOC Range
341-450 g/L
Industry
Railcar Industry
Exposure
Exterior Weathering, UV, General Industrial
Substrate
Steel Locomotive
Tradename
VpCI-396Z/395/2026
System
Organic Zinc/Epoxy Novolac/Epoxy Novolac
VOC Range
341-450 g/L
Industry
Power Plants
Exposure
Chemical/Water Exposure - Caustic or Acid
Substrate
Steel
Tradename
VpCI-396Z/396/384
System
Organic Zinc/Urethane/Urethane
VOC Range
341-450 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Steel