JPCL Coatings & Linings Buying Guide Back to Superstore Home

Comment |
Company Details

Termarust Technologies Inc.
7726 rue Jarry East
Montreal QC H1J 2M3 Canada

Contact for sales inquiries: Wayne Senick
Phone number for sales inquiries: 888-279-5497 ext 221
Fax number for sales inquiries: 514-354-2799

 

5 recommended systems for All Industries; All Exposures; All Substrates

Tradename
Termarust TR2000 HRCSA series
System
Calcium Sulphonate
VOC Range
101-250 g/L
Industry
Transmission Pipeline
Exposure
Above Ground Pipe Exteriors
Substrate
Steel
 
Tradename
Termarust TR2000 HRCSA series
System
Calcium Sulphonate
VOC Range
<100 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Marine Industry; Offshore Industry; Power Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Ballast Tank Linings; Chemical/Water Exposure - Wet Fly Ash; Circulating Water Pipe; Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe; Exterior Weathering, UV, and Mild Chemical; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Severe Wet End Exposure - Paper Machines; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion; Topsides [Severe Marine Exposure]
Substrate
Concrete; Steel
 
Tradename
Termarust TR2000 HRCSA Series
System
Calcium Sulphonate
VOC Range
101-250 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Marine Industry; Offshore Industry; Power Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Ballast Tank Linings; Chemical/Water Exposure - Wet Fly Ash; Circulating Water Pipe; Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe; Exterior Weathering, UV, and Mild Chemical; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Severe Wet End Exposure - Paper Machines; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion; Topsides [Severe Marine Exposure]
Substrate
Concrete; Steel
 
Tradename
Termarust TR2000 HRCSA series;
System
Calcium Sulphonate
VOC Range
101-250 g/L
Industry
Offshore Industry
Exposure
Jacket [Splash Zone; Atmospheric Zone]
Substrate
Steel
 
Tradename
Termarust TR2100 HRCSA series
System
Calcium Sulphonate
VOC Range
101-250 g/L
Industry
Marine Industry
Exposure
Interior Mild
Substrate
Steel