JPCL Coatings & Linings Buying Guide Back to Superstore Home

Comment |
Company Details

Andek Corporation
850 Glen Ave., PO Box 392
Moorestown NJ 08057 USA

Contact for sales inquiries: Neil Shearer
Phone number for sales inquiries: 800-800-2844
Fax number for sales inquiries: 856-786-0580

 

20 recommended systems for All Industries; All Exposures; All Substrates

Tradename
AIM#1
System
Urethane Elastomeric (1 Coat)
VOC Range
101-250 g/L
Industry
Transmission Pipeline
Exposure
External of Buried Pipe
Substrate
Concrete; Steel
 
Tradename
Andek Industrial Membrane #1
System
Urethane/Urethane
VOC Range
101-250 g/L
Industry
Water Works
Exposure
Immersion Exposure - Non-Potable Water
Substrate
Concrete
 
Tradename
Andek Wearcoat 66
System
Urethane/Urethane
VOC Range
251-340 g/L
Industry
Marine Industry
Exposure
Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]
Substrate
Steel
 
Tradename
Andek Where Coat 66
System
Urethane/Urethane
VOC Range
251-340 g/L
Industry
Bridges; Water Works
Exposure
Exterior Exposure - Weathering and UV; Exterior Weathering - Severe
Substrate
Concrete; Steel
 
Tradename
Cocoon 501
System
Vinyl Ester/Vinyl Ester/Vinyl Ester
VOC Range
251-340 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper
Exposure
Interior Dry Exposure; Interior Process Areas
Substrate
Concrete Walls, Ceilings
 
Tradename
Cocoon 550
System
Vinyl Ester/Vinyl Ester/Vinyl Ester
VOC Range
251-340 g/L
Industry
Chemical & Petrochemical Plants; Transmission Pipeline; Wastewater Treatment Plants, Municipal
Exposure
Above Ground Pipe Exteriors; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete; Steel
 
Tradename
Cocoon 560
System
Vinyl Ester/Vinyl Ester/Vinyl Ester
VOC Range
Industry
Pulp & Paper; Water Works
Exposure
Immersion Exposure - Non-Potable Water; Interior Normal Wet Exposure
Substrate
Concrete; Steel
 
Tradename
Cocoon 560
System
Vinyl Ester/Vinyl Ester/Vinyl Ester
VOC Range
251-340 g/L
Industry
Pulp & Paper; Water Works
Exposure
Immersion Exposure - Non-Potable Water; Interior Normal Wet Exposure
Substrate
Concrete; Steel
 
Tradename
Encapsal Super
System
Urethane/Urethane
VOC Range
101-250 g/L
Industry
Wastewater Treatment Plants, Municipal
Exposure
Interior Exposure Environment
Substrate
Concrete Walls, Ceilings
 
Tradename
Flashband
System
Tape Wraps
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate
Substrate
Steel
 
Tradename
IMCAS ESP2
System
Sheet Lining, Thermoplastic
VOC Range
251-340 g/L
Industry
Power Plants
Exposure
FGD Interiors
Substrate
Steel
 
Tradename
Polacav
System
Sheet Lining, Thermoplastic
VOC Range
251-340 g/L
Industry
Wastewater Treatment Plants, Municipal; Waterfont, Lock, and Dam Industry
Exposure
Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Freshwater
Substrate
Concrete; Steel
 
Tradename
Polafloor Epoxy Topping
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper
Exposure
Interior Dry Exposure; Interior Process Areas
Substrate
Concrete Floors
 
Tradename
Polafloor Epoxy Toppping
System
Epoxy Surfacer (two-part)
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Concrete Surfacing Materials
Substrate
 
Tradename
Polafloor PUR
System
Polyurea Hybrid (1, 2, or 3 coats)
VOC Range
<100 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Power Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Exterior Weathering - Severe; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Process Water, Brine, Waste Water]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
Polafloor PUR
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Power Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Exterior Weathering - Severe; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Process Water, Brine, Waste Water]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
Polagard AG
System
Epoxy/Urethane (color)/Urethane (clear)
VOC Range
251-340 g/L
Industry
Chemical & Petrochemical Plants; Specialty Functions; Wastewater Treatment Plants, Municipal
Exposure
Anti-Graffiti; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete; Steel
 
Tradename
Polagard AG
System
Urethane/Urethane
VOC Range
251-340 g/L
Industry
Chemical & Petrochemical Plants; Specialty Functions; Wastewater Treatment Plants, Municipal
Exposure
Anti-Graffiti; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete; Steel
 
Tradename
Polaprime 21
System
Corrosion Protection
VOC Range
251-340 g/L
Industry
Specialty Functions
Exposure
Conversion Coatings
Substrate
 
Tradename
Polaseal MA
System
Siloxane/Siloxane
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate
Substrate
Concrete