Company Details
Normac Adhesive Products Inc.
|
1350 Heine Court |
Burlington ON L7L 6M4 Canada
|
Contact for sales inquiries:
Mark Cussons, Steve Gates, George MacGregor
|
Phone number for sales inquiries: 905-332-6455 |
Fax number for sales inquiries: 905-332-6880 |
10 recommended systems for All Industries; All Exposures; All Substrates
Tradename
LVHS
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; Exterior Exposure - Weathering and UV; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Secondary Containment
Substrate
Concrete; Steel
Tradename
LVHS Series
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Transmission Pipeline
Exposure
External of Buried Pipe; Field Joint Coating of Buried Pipe
Substrate
Concrete; Steel
Tradename
NR=95LVHS, NR-80LVHS
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Wastewater Treatment Plants, Municipal
Exposure
Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment
Substrate
Concrete
Tradename
NR-5S 400
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Primary Containment (Nuclear Only)
Substrate
Tradename
NR-80/95LVHS
System
Urethane/Urethane
VOC Range
Industry
Bridges; Pulp & Paper; Railcar Industry; Transmission Pipeline
Exposure
Chemical Exposure - Caustic; Exterior Weathering - Severe; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Concrete; Livestock Carriers; Steel
Tradename
NR-80/95LVHS
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Bridges; Pulp & Paper; Railcar Industry; Transmission Pipeline
Exposure
Chemical Exposure - Caustic; Exterior Weathering - Severe; Internal of Buried Pipe; Linings for Steel Rail Car Interiors
Substrate
Concrete; Livestock Carriers; Steel
Tradename
NR-80LVHS
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Marine Industry
Exposure
Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]
Substrate
Steel
Tradename
NR-80LVHS, NR-95LVHS
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Food/Beverage & Pharmaceutical Plants; Marine Industry; Offshore Industry; Power Plants; Pulp & Paper; Railcar Industry
Exposure
Ballast Tank Linings; Below Water Line; Cargo Hold Linings; Cargo Tank Linings; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; Circulating Water Pipe; Interior Mild; Interior Normal Wet Exposure; Interior Process Areas; Linings for Steel Rail Car Interiors; Linings for Steel Storage Tanks & Vessels [Process Water, Brine, Waste Water]; Secondary Containment; Topsides [Severe Marine Exposure]
Substrate
Bulk Solids; Concrete; Concrete Floors; Concrete Walls, Ceilings; Steel
Tradename
NR-95LVHS
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Wastewater Treatment Plants, Municipal
Exposure
Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment
Substrate
Steel
Tradename
NR-95LVHS, NR-80LVHS
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Immersion - Tertiary Treatment; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Immersion Exposure - Seawater; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Concrete; Steel