20 recommended systems for All Industries; All Exposures; All Substrates
Tradename
Ply-Guard AS Polyaspartic
System
Polyurea Hybrid (1, 2, or 3 coats)
VOC Range
<100 g/L
Industry
Bridges; Transmission Pipeline; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; Exterior Exposure - Weathering and UV; Exterior Weathering - Severe; Immersion Exposure - Freshwater; Immersion Exposure - Seawater; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Concrete; Steel
Tradename
Ply-Guard EP (Novolac) Epoxy
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Power Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Chemical Exposure - Acid; Chemical/Water Exposure - Caustic or Acid; Secondary Containment
Substrate
Concrete
Tradename
Ply-Guard EP Epoxy
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Interior Dry Exposure; Interior Exposure Environment; Interior Process Areas
Substrate
Concrete Floors
Tradename
Ply-Guard EP Epoxy (Walls)
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Interior Dry Exposure; Interior Exposure Environment; Interior Process Areas
Substrate
Concrete Walls, Ceilings
Tradename
Ply-Guard EP Epoxy (Walls)
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Interior Dry Exposure; Interior Exposure Environment; Interior Process Areas
Substrate
Concrete Walls, Ceilings
Tradename
Ply-Guard EP/Ply-Guard EP (Novolac) Epoxy
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Power Plants
Exposure
Secondary Containment
Substrate
Concrete
Tradename
Ply-Guard UR
System
Polyurea Pure (1, 2, or 3 coats)
VOC Range
<100 g/L
Industry
Bridges; Chemical & Petrochemical Plants
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Exterior Weathering - Mild/Moderate
Substrate
Concrete
Tradename
Ply-Guard UR (Polyurea)/Ply-Guard AS (Polyaspartic)
System
Polyurea Pure (1, 2, or 3 coats)
VOC Range
<100 g/L
Industry
Wastewater Treatment Plants, Municipal
Exposure
Exterior Weathering, UV, and Mild Chemical
Substrate
Concrete; Steel
Tradename
Ply-Guard UR (Potable Water) Polyurea
System
Polyurea Pure (1, 2, or 3 coats)
VOC Range
<100 g/L
Industry
Water Works
Exposure
Immersion Exposure - Potable Water Approved
Substrate
Concrete; Steel
Tradename
Ply-Guard UR Polyurea
System
Polyurea Pure (1, 2, or 3 coats)
VOC Range
<100 g/L
Industry
Power Plants; Pulp & Paper; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works
Exposure
Above Ground Pipe Exteriors; Chemical Exposure - Acid; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; Circulating Water Pipe; External of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Non-Potable Water; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Severe Wet End Exposure - Paper Machines
Substrate
Concrete; Concrete Floors; Steel
Tradename
WB HRZS® PCP
System
Inorganic Zinc
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Shop Primers for Steel
Substrate
Tradename
WB HRZS® Primer / Ply-Guard AS Polyaspartic
System
Inorganic Zinc/Polyurea Hybrid
VOC Range
<100 g/L
Industry
Marine Industry; Railcar Industry
Exposure
Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, General Industrial; Interior Mild
Substrate
Steel; Steel Locomotive; Steel Rail Cars
Tradename
WB HRZS® Primer / Ply-Guard UR
System
Inorganic Zinc/Polyurea (Pure)
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Livestock Carriers
Tradename
WB HRZS® Primer / Ply-Guard UR (Potable Water)
System
Inorganic Zinc/Polyurea (Pure)
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Dairy
Tradename
WB HRZS® Primer / Ply-Guard UR (XTS)
System
Inorganic Zinc/Polyurea (Pure)
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Linings for Steel Rail Car Interiors
Substrate
Acids; Alkalis; Bulk Solids
Tradename
WB HRZS® Primer + Ply-Guard PSC8 Polysiloxane
System
Inorganic Zinc/Epoxy/Siloxane
VOC Range
<100 g/L
Industry
Offshore Industry
Exposure
Topsides [Severe Marine Exposure]
Substrate
Steel
Tradename
WB HRZS® Primer/Ply Guard AS
System
Inorganic Zinc/Polyurea Hybrid
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Severe
Substrate
Steel
Tradename
WB HRZS® Primer/Ply-Guard AS
System
Inorganic Zinc/Polyurea Hybrid
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate
Substrate
Steel
Tradename
WB HRZS® Primer/Ply-Guard AS Polyaspartic
System
Inorganic Zinc/Polyurea Hybrid
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali]
Substrate
Steel
Tradename
WB HRZS® Single Coat System
System
Zinc-rich, inorganic
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Marine Industry; Offshore Industry; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Ballast Tank Linings; Below Water Line; Cargo Hold Linings; Cargo Tank Linings; Exterior Exposure - Weathering and UV; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Immersion Exposure - Seawater; Jacket [Immersed Area; Splash Zone; Atmospheric Zone]; Linings for Steel Storage Tanks & Vessels [Process Water, Brine, Waste Water]; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Steel