JPCL Coatings & Linings Buying Guide Back to Superstore Home

Comment |
Company Details

Master Builders Solutions
889 Valley Park Dr.
Shakopee MN 55379 USA

Contact for sales inquiries: Customer Service
Phone number for sales inquiries: 800-433-9517
Fax number for sales inquiries:

 

5 recommended systems for All Industries; All Exposures; All Substrates

Tradename
MasterBrace 6000
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Offshore Industry
Exposure
Jacket [Immersed Area; Splash Zone]
Substrate
Steel
 
Tradename
MasterBrace 6000 UW
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Marine Industry
Exposure
Below Water Line
Substrate
Steel
 
Tradename
MasterProtect H 400
System
Siloxane/Siloxane
VOC Range
341-450 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate
Substrate
Concrete
 
Tradename
MasterSeal 350
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Severe
Substrate
Concrete
 
Tradename
UCRETE
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants
Exposure
Interior Process Areas
Substrate
Concrete Floors