30 recommended systems for All Industries; All Exposures; All Substrates

Tradename
AWR Super Sealer
System
Methyl Methacrylate/Methyl Methacrylate
VOC Range
<100 g/L
Industry
Pulp & Paper; Wastewater Treatment Plants, Municipal
Exposure
Interior Dry Exposure; Interior Exposure Environment
Substrate
Concrete Floors
 
Tradename
Bio-SAFE MaxLife
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate
Substrate
Concrete
 
Tradename
Bio-SAFE Prime & Seal/MaxLife
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; Exterior Exposure - Weathering and UV; Exterior Weathering, UV, and Mild Chemical; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt
Substrate
Concrete; Concrete Walls, Ceilings
 
Tradename
Bio-SAFE Prime & Seal/MaxLife
System
Epoxy (1-2 coats)/Acrylic (1-2 coats)
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Pulp & Paper; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; Exterior Exposure - Weathering and UV; Exterior Weathering, UV, and Mild Chemical; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt
Substrate
Concrete; Concrete Walls, Ceilings
 
Tradename
Bio-SAFE Prime & Seal/Super Urethane
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Chemical Exposure - Acid; Secondary Containment
Substrate
Concrete
 
Tradename
Bio-SAFE Prime & Seal/Super Urethane
System
Urethane/Urethane
VOC Range
101-250 g/L
Industry
Pulp & Paper
Exposure
Chemical Exposure - Acid; Secondary Containment
Substrate
Concrete
 
Tradename
Bio-SAFE System
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Chemical/Water Exposure - Caustic or Acid
Substrate
Concrete
 
Tradename
Bio-Safe/DeckMaster
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Chemical/Water Exposure - Wet Fly Ash
Substrate
Steel
 
Tradename
RUSTOP 6000 System
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Marine Industry
Exposure
Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]
Substrate
Steel
 
Tradename
RUSTOP 6000/Graf Max
System
Urethane/Urethane
VOC Range
341-450 g/L
Industry
Food/Beverage & Pharmaceutical Plants
Exposure
Interior Process Areas
Substrate
Concrete Floors
 
Tradename
RUSTOP Aluminim Urethane
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Waterfont, Lock, and Dam Industry
Exposure
Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Steel
 
Tradename
RUSTOP Aluminum Urethane
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Railcar Industry; Waterfont, Lock, and Dam Industry
Exposure
Linings for Steel Rail Car Interiors; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion
Substrate
Bulk Solids; Concrete; Livestock Carriers
 
Tradename
RUSTOP Maximum
System
Epoxy (fast dry, extended recoat)
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Shop Primers for Steel
Substrate
 
Tradename
RUSTOP Maximum/SP-X Silicone Poly Plus
System
Silicone Modified/Silicone Modified
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Heat-Resistant Coatings [Dry Heat Resistance from 201 F to 450 F (99 C to 233 C); Dry Heat Resistance from 451 F to 800 F (234 C to 427 C); Under Insulation, Wet Heat Resistance up to 300 F (149 C)]
Substrate
Steel
 
Tradename
RUSTOP Metallic
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Power Plants
Exposure
Chemical/Water Exposure - Wet Fly Ash
Substrate
Concrete
 
Tradename
RUSTOP Metallic 6000
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Power Plants; Wastewater Treatment Plants, Municipal
Exposure
Secondary Containment
Substrate
Concrete
 
Tradename
RUSTOP Metallic 6000
System
Urethane/Urethane
VOC Range
101-250 g/L
Industry
Chemical & Petrochemical Plants; Power Plants; Wastewater Treatment Plants, Municipal
Exposure
Secondary Containment
Substrate
Concrete
 
Tradename
RUSTOP Metallic Urethane/Super Urethane
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Railcar Industry
Exposure
Exterior Weathering, UV, General Industrial
Substrate
Steel Rail Cars
 
Tradename
RUSTOP/ Bio-SAFE MaxLife
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Severe
Substrate
Steel
 
Tradename
RUSTOP/Bio-SAFE
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Severe
Substrate
Concrete
 
Tradename
RUSTOP/Bio-SAFE MaxLife
System
Alkyd/Acrylic/Acrylic
VOC Range
<100 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Marine Industry
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering - Mild/Moderate; Interior Mild
Substrate
Concrete; Steel
 
Tradename
RUSTOP/Bio-SAFE MaxLife
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Bridges; Chemical & Petrochemical Plants; Marine Industry
Exposure
Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering - Mild/Moderate; Interior Mild
Substrate
Concrete; Steel
 
Tradename
RUSTOP/Graffiti Max
System
Epoxy/Urethane (color)/Urethane (clear)
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Anti-Graffiti
Substrate
Concrete; Steel
 
Tradename
RUSTOP/MaxLife
System
Other
VOC Range
Industry
Power Plants
Exposure
Circulating Water Pipe
Substrate
Steel
 
Tradename
RUSTOP/Silicone Poly Plus
System
Epoxy (1-2 coats)/Urethane
VOC Range
<100 g/L
Industry
Transmission Pipeline; Wastewater Treatment Plants, Municipal
Exposure
Above Ground Pipe Exteriors; Exterior Weathering, UV, and Mild Chemical
Substrate
Steel
 
Tradename
RUSTOP/SP-50 Silicone Poly Plus
System
Epoxy (1-2 coats)/Urethane
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Water Works
Exposure
Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Steel
 
Tradename
RUSTOP/SP-50 Silicone Poly Plus
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Water Works
Exposure
Exterior Exposure - Weathering and UV; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV]
Substrate
Steel
 
Tradename
RUSTOP/SP-X Silicone Poly Plus
System
Epoxy (1-2 coats)/Urethane
VOC Range
<100 g/L
Industry
Offshore Industry; Power Plants; Pulp & Paper; Railcar Industry; Wastewater Treatment Plants, Municipal; Waterfont, Lock, and Dam Industry
Exposure
Chemical Exposure - Acid; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Exterior Weathering, UV, General Industrial; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Jacket [Atmospheric Zone]; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Topsides [Severe Marine Exposure]
Substrate
Steel; Steel Locomotive
 
Tradename
Silox Seal/Prime & Seal 1,2,3
System
Other Special Block Filler
VOC Range
<100 g/L
Industry
Specialty Functions
Exposure
Concrete Surfacing Materials
Substrate
 
Tradename
Super Urethane/Graf Max
System
Urethane/Urethane
VOC Range
<100 g/L
Industry
Pulp & Paper
Exposure
Chemical Exposure - Caustic
Substrate
Concrete