10 recommended systems for All Industries; All Exposures; All Substrates

Tradename
CHEMCLAD
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Food/Beverage & Pharmaceutical Plants; Marine Industry; Offshore Industry; Power Plants; Pulp & Paper; Railcar Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; Below Water Line; Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Acid; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; Circulating Water Pipe; Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; External of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Immersion Exposure - Potable Water Approved; Immersion Exposure - Seawater; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas; Interior Severe Wet End Exposure - Paper Machines; Internal of Buried Pipe; Jacket [Splash Zone; Atmospheric Zone]; Linings for Steel Rail Car Interiors; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Primary Containment (Nuclear Only); Secondary Containment; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion; Topsides [Severe Marine Exposure]
Substrate
; Acids; Alkalis; Bulk Solids; Concrete; Concrete Floors; Concrete Walls, Ceilings; Dairy; Hydrocarbons; Livestock Carriers; Steel
 
Tradename
CHEMCLAD
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Food/Beverage & Pharmaceutical Plants; Marine Industry; Offshore Industry; Power Plants; Pulp & Paper; Railcar Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; Below Water Line; Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Acid; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; Circulating Water Pipe; Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; External of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Immersion Exposure - Potable Water Approved; Immersion Exposure - Seawater; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas; Interior Severe Wet End Exposure - Paper Machines; Internal of Buried Pipe; Jacket [Splash Zone; Atmospheric Zone]; Linings for Steel Rail Car Interiors; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Primary Containment (Nuclear Only); Secondary Containment; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion; Topsides [Severe Marine Exposure]
Substrate
; Acids; Alkalis; Bulk Solids; Concrete; Concrete Floors; Concrete Walls, Ceilings; Dairy; Hydrocarbons; Livestock Carriers; Steel
 
Tradename
CHEMCLAD
System
Epoxy/Epoxy 100% solids
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Food/Beverage & Pharmaceutical Plants; Marine Industry; Offshore Industry; Power Plants; Pulp & Paper; Railcar Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; Below Water Line; Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Acid; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; Circulating Water Pipe; Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; External of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Immersion Exposure - Potable Water Approved; Immersion Exposure - Seawater; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas; Interior Severe Wet End Exposure - Paper Machines; Internal of Buried Pipe; Jacket [Splash Zone; Atmospheric Zone]; Linings for Steel Rail Car Interiors; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Primary Containment (Nuclear Only); Secondary Containment; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion; Topsides [Severe Marine Exposure]
Substrate
; Acids; Alkalis; Bulk Solids; Concrete; Concrete Floors; Concrete Walls, Ceilings; Dairy; Hydrocarbons; Livestock Carriers; Steel
 
Tradename
CHEMCLAD
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Food/Beverage & Pharmaceutical Plants; Marine Industry; Offshore Industry; Power Plants; Pulp & Paper; Railcar Industry; Transmission Pipeline; Wastewater Treatment Plants, Municipal; Water Works; Waterfont, Lock, and Dam Industry
Exposure
Above Ground Pipe Exteriors; Below Water Line; Cargo Hold Linings; Cargo Tank Linings; Chemical Exposure - Acid; Chemical Exposure - Caustic; Chemical/Water Exposure - Caustic or Acid; Chemical/Water Exposure - Wet Fly Ash; Circulating Water Pipe; Exterior Deck Plate [Abrasion, Marine, Weathering, & UV]; Exterior Exposure - Weathering and UV; Exterior Superstructures [Marine, Weathering, & UV]; Exterior Weathering, UV, and Mild Chemical; External of Buried Pipe; Immersion - Tertiary Treatment; Immersion - Wastewater Collection, Primary Treatment, Secondary Treatment; Immersion Exposure - Freshwater; Immersion Exposure - Non-Potable Water; Immersion Exposure - Potable Water Approved; Immersion Exposure - Seawater; Interior Dry Exposure; Interior Exposure Environment; Interior Normal Wet Exposure; Interior Process Areas; Interior Severe Wet End Exposure - Paper Machines; Internal of Buried Pipe; Jacket [Splash Zone; Atmospheric Zone]; Linings for Steel Rail Car Interiors; Onshore Atmospheric Exposure - Weathering, UV, & Airborne Salt; Primary Containment (Nuclear Only); Secondary Containment; Splash Zone Exposure - Weathering, UV, Fresh or Saltwater Splash, & Abrasion; Topsides [Severe Marine Exposure]
Substrate
; Acids; Alkalis; Bulk Solids; Concrete; Concrete Floors; Concrete Walls, Ceilings; Dairy; Hydrocarbons; Livestock Carriers; Steel
 
Tradename
CHEMCLAD SC
System
Epoxy 100% Solids (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants
Exposure
Linings for Steel Storage Tanks & Vessels [Process Water, Brine, Waste Water]
Substrate
Steel
 
Tradename
CHEMCLAD XC
System
Epoxy Novolac (1 or 2 Coats)
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Power Plants
Exposure
Chemical/Water Exposure - Caustic or Acid; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV; Chemical, Weathering, & UV]; FGD Interiors; FGD Stack Interiors; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
CHEMCLAD XC
System
Epoxy/Epoxy Novolac/Epoxy Novolac
VOC Range
<100 g/L
Industry
Chemical & Petrochemical Plants; Power Plants
Exposure
Chemical/Water Exposure - Caustic or Acid; Exterior Plant Exposure - Moderate to Severe [Chemical, Weathering, & UV; Chemical, Weathering, & UV]; FGD Interiors; FGD Stack Interiors; Linings for Steel Storage Tanks & Vessels [Solvents, Jet Fuel, Diesel, Gasoline, Crude Oil; Acid, Oxidizer, Alkali]; Secondary Containment
Substrate
Concrete; Steel
 
Tradename
ENESEAL
System
Other
VOC Range
<100 g/L
Industry
Bridges
Exposure
Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe
Substrate
Concrete
 
Tradename
ENESEAL CR
System
Other
VOC Range
<100 g/L
Industry
Bridges; Marine Industry; Railcar Industry
Exposure
Exterior Weathering - Mild/Moderate; Exterior Weathering - Severe; Exterior Weathering, UV, General Industrial; Interior Mild
Substrate
Steel; Steel Rail Cars
 
Tradename
ENESEAL HR
System
Other
VOC Range
<100 g/L
Industry
Food/Beverage & Pharmaceutical Plants; Transmission Pipeline
Exposure
Above Ground Pipe Exteriors; Interior Process Areas