This JPCL Collection edition includes eight articles, originally published in JPCL, by experts in coating technology.
The Development of Corrosion Resistant 2- and 1-K Waterbased Zinc-Rich Paints
JPCL July 2017 - J. Peter Ault, P.E., PCS and Eric Shoyer, Elzly Technology Corporation
Low-VOC High-Performance Waterborne Epoxy Systems in Protective Coating Application
JPCL January 2017 - Yong Zhang, Olin Epoxy, Olin Corporation
All Silicones are Not Created Equal
JPCL March 2016 - Gerald L. Witucki, Dow Corning Corporation
The Negative Influence of Fe2P Pigments on the Anti-Corrosion Properties of Zinc Dust Primers
JPCL December 2015 - Pascal Verbiest, Dr. Sc., Umicore Zinc Chemicals
Encouraging Innovation: Environmental Regulations Drive Epoxy Formulation
JPCL April 2015 - Marcelo Rufo, Air Products and Chemicals, Inc.
Coatings for the Oil & Gas Market: A Simplified Approach to Formulating for High-Temperature and High-Pressure Applications
JPCL March 2015 - Andrew Recker, BASF
FEVE Technology for Higher Performance Coating Systems on Bridges
JPCL January 2015 - Bob Parker, AGC Chemicals Americas, Inc.
Improving Polyurethane Pipe Coatings for Harsh Conditions
JPCL August 2014 - Andreas aus der Wieschen, Matthias Wintermantel, Todd Williams and Ahren Olson, Bayer MaterialScience AG
The full color print edition of this JPCL Collection is available for purchase in the TPC Store.
|