This JPCL Collection edition includes seventeen articles, originally published in JPCL, by experts in surface preparation.
Surface Preparation: A Continuing Evolution JPCL Three Decades of Change in the Coatings Industry 2013 Special Issue - Charles Lange, JPCL
Why surface preparation is important
JPCL May 2013 - Robert Barnhart, Debbie Mericle, Chuck Mobley, Tom Hocking, Jeff Bogran, and Ernestine McDaniel
Preparing Concrete Floors for Coatings
JPCL January 2013 - Tracey Glew, The Preparation Group
Preparing stainless steel for atmospheric salt service
JPCL October 2012
What is a Green Abrasive?
JPCL October 2012 - David Dorrow, Mineral Aggregates Inc.
Preparing Surfaces at Wastewater Plants: An Overview of Substrates, Practices, and Standards
JPCL September 2012 - Vaughn O’Dea, Tnemec Company, Inc.
Six Key Points You Should Know about Concrete Surface Preparation before Coating Application
JPCL July 2012 - Fred Goodwin, BASF Construction Chemicals
Characterizing Surfaces after UHP Waterjetting in New Ship Construction
JPCL May 2011 - Philippe Le Calvé, DCNS, France; Jean-Pierre Pautasso, Direction Générale de I’Armement, France; and Nathalie Le Bozec, French Corrosion Institute
Using Robots in Ballast Tanks: Project Under Way to Automate Inspection of Surface Prep and Coating Work
JPCL January 2011 - Lars-Eric Etzold, Meyer Werft GmbH
How Does Waterjet Cleaning Affect the Surface and Surface Preparation?
JPCL January 2010 - Lydia M. Frenzel, Ph.D., Advisory Council