E376 Standard Practice for Measuring Coating Thickness by Magnetic-Field or Eddy-Current (Electromagnetic) Examination Methods

All Standards | ASTM Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
1.1 This practice covers the use of magnetic- and eddy-current-type thickness instruments (gages) for nondestructive thickness measurement of a coating on a metal substrate.

1.2 More specific uses of these instruments are covered by the following test methods issued by ASTM: Test Methods B 244, B 499, B 530, D 1186, D 1400, and G 12.

1.3 The values stated in SI units are to be regarded as standard. The inch-pound units in parentheses are for information only and may be approximate.

1.4 Measurements made in accordance with this test method will be in compliance with the requirements of ISO International Standard 2178 as printed in 1982.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

(Back to all Standards)

 
   
Advertisements
 
EDCO - Equipment Development Co. Inc.

 
Tarps manufacturing, Inc.

 
CRW

 
Strand’s Industrial Coatings

 
Sauereisen, Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Axxiom Manufacturing

 
HoldTight Solutions Inc.

 
Abrasives Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us