NACE No. 11/SSPC-PA 8 NACE No. 11/SSPC-PA 8 Thin-Film Organic Linings Applied in New Carbon Steel Process Vessels

All Standards | NACE Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: July 18, 2012
Editorial Change:
 
New in 2003! Specifies procedures to design, install, and inspect thin-film organic linings applied to new carbon steel process vessels to prevent corrosion and other forms of degradation, such as hydrogen-induced cracking, or to prevent product contamination. It is also useful for lining applications in existing process vessels and equipment. Based on applications of organic linings 500 µm (20 mils) or less. Useful for lining vessels in many industries including, but not limited to, refining, chemical, water-treating, and food. The intended users are owners, contractors, inspectors, applicators, vessel designers, protective coatings specialists, and others concerned with the lining of process vessels.

(Back to all Standards)

 
   
Advertisements
 
Abrasives Inc.

 
HoldTight Solutions Inc.

 
KTA-Tator, Inc. - Corporate Office

 
Sauereisen, Inc.

 
CRW

 
Axxiom Manufacturing

 
PaintSquare

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us