ISO 7539-4:1989 ISO 7539-4:1989 Corrosion of metals and alloys -- Stress corrosion testing -- Part 4: Preparation and use of uniaxially loaded tension specimens

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Covers procedures for designing, preparing and using uniaxially loaded tension specimens. These specimens may be used to test a variety of product forms (for example sheet, plate, tubes, wire or rod as well as parts joined by welding, riveting, or other methods). Uniaxially loaded tensile specimens may be stressed quantitatively with equipment for application of either a constant load, a constant strain or an increasing load or strain.

(Back to all Standards)

 
   
Advertisements
 
Fischer Technology Inc.
 
Maximize Profits by Monitoring Coating Thickness
 
Learn more by contacting Fischer Technology today: 1.860.683.0781
 

 
DeFelsko Corporation
 
PosiTector SST Soluble Salt Tester
 
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.
 

 
Norton Sandblasting Equipment
 
Norton Sandblasting Equipment
 
We are a premier stocking distributor for the leading manufacturers of surface preparation equipment, industrial dust collection, vacuums and more.
 

 
Sika-Us
 
Sika® Industrial Floor Coatings
 
Click to learn about floor and wall systems relied upon for performance, durability, easy maintenance and aesthetics across the every industry and environment.
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
Sauereisen, Inc.
 
Substrate Repair Materials
 

Substrate Repair Materials and Filler Compounds

Sauereisen's full line of underlayments are the ideal substrate repair materials to restore structural integrity prior to the application of SewerGard©
 

 
Sidewinder/Persyst Enterprises, Inc.
 
Sidewinder Model M2
 
Load our Refrigeration Machine Distiller Reclaimer with dirty solvent, press the button, you're done. You will have clean gun wash and cleanup solvents, ready for reuse.
 

 
SABRE Autonomous Solutions
 
Introducing the ALPHA1 Blasting Robot
 
Once installed and commissioned – simply
SCAN PLAN BLAST.
 

 
CS Unitec
 
Dust Control Surface Prep Industrial Tools for Steel and Concrete
 
Scarifying • Grinding Scabbling • Descaling Dust collection for safer working conditions. Low-vibration for less worker fatigue. Trelawny™ power tools from CS Unitec. Learn more…
 

 
US Minerals
 
Blast with the best
 
The most effective blasting media on the market, Black Diamond hits harder and cleans faster.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us