ISO 7441:1984 ISO 7441:1984 Corrosion of metals and alloys -- Determination of bimetallic corrosion in outdoor exposure corrosion tests

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Applies to metals and alloys, and metals and alloys with metallic and non-metallic non-organic coatings. The methods are intended for the determination of the amount and type of corrosion effect, arising in natural atmospheres, caused by contact with different metals (coated metals), and for the evaluation of the effectiveness of bimetallic corrosion protection treatments.

(Back to all Standards)

 
   
Advertisements
 
Modern Safety Techniques

 
Strand’s Industrial Coatings

 
Paint BidTracker

 
HoldTight Solutions Inc.

 
NLB Corporation

 
Tarps manufacturing, Inc.

 
Sauereisen, Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us