ISO 8079:1984 ISO 8079:1984 Aerospace process -- Anodic treatment of aluminium alloys -- Sulfuric acid process, dyed coating

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Includes requirements for producing and testing a coating on aluminium alloys where the coating is not required to withstand prolonged exposure to weathering and direct sunlight. The anodizing process is applied in the manufacture of aerospace products to improve resistance to corrosion, produce coloured surfaces for aesthetic reasons or to colour code parts for identification purposes.

(Back to all Standards)

 
   
Advertisements
 
KTA-Tator, Inc. - Corporate Office
 
KTA-Tator Training Course Opportunities
 
• IACET Authorized Continuing Education Unit (CEU) Provider
• Live Basic Coatings Inspection Courses
• Customized/Private Courses
• Online/self-paced curriculums
Contact: Tiffany Kelly at 412-788-1300 x217
 

 
ARC / A.W. Chesterton Company
 
Rapid Curing Coating
 
Cures under adverse conditions with maximum adhesion
 

 
SABRE Autonomous Solutions
 
Productivity
 
Personnel are free to do other tasks while the ALPHA1 does the “dirty work”.
 

 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
 

 
HoldTight Solutions Inc.
 
Full Surface Protection for Up to One Year
 
HT 365 is a preservation, single component, anti-corrosive coating, a water displacing agent, a lubricant, and a penetrating fluid. It creates an imperceptible thin-film coating that offers excellent salt contaminant and humidity protection. Contact your HoldTight® representative or visit Holdtight.com for more information.
 

 
DeFelsko Corporation
 
PosiTector SHD Shore Hardness Durometer
 
PosiTector SHD measures the hardness of non-metallic materials. Features a measurement timer, auto ignore mode and internal memory. Shore A or D available.
 

 
Fischer Technology Inc.
 
Maximize Profits by Monitoring Coating Thickness
 
Learn more by contacting Fischer Technology today: 1.860.683.0781
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us