ISO 9220:1988 ISO 9220:1988 Metallic coatings -- Measurement of coating thickness -- Scanning electron microscope method

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Specifies a method for the measurement of the local thickness of metallic coatings by examination of cross-section with a scanning electron microscope. It is destructive and has an uncertainty of less than 10 % or 0,1 /um, whichever is greater. It can be used for thicknesses up to several millimetres, but it is usually more practical to use a ligth microscope (ISO 1463). Annex a gives the preparation of cross-sections.

(Back to all Standards)

 
   
Advertisements
 
Sauereisen, Inc.
 
Substrate Repair Materials
 

Substrate Repair Materials and Filler Compounds

Sauereisen's full line of underlayments are the ideal substrate repair materials to restore structural integrity prior to the application of SewerGard©
 

 
DeFelsko Corporation
 
PosiTector SST Soluble Salt Tester
 
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.
 

 
CS Unitec
 
Dust Control Surface Prep Industrial Tools for Steel and Concrete
 
Scarifying • Grinding Scabbling • Descaling Dust collection for safer working conditions. Low-vibration for less worker fatigue. Trelawny™ power tools from CS Unitec. Learn more…
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
US Minerals
 
Blast with the best
 
The most effective blasting media on the market, Black Diamond hits harder and cleans faster.
 

 
Norton Sandblasting Equipment
 
Norton Sandblasting Equipment
 
We are a premier stocking distributor for the leading manufacturers of surface preparation equipment, industrial dust collection, vacuums and more.
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us