SSPC-Paint 32, Coal Tar Emulsion Coating

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: April 01, 2006
Updated On: April 01, 2002
Editorial Change: April 1, 2006
 
This specification covers a coal tar emulsion coating to be used as a protective weather coat for hot or cold applied bituminous coatings on steel structures. It may also be used over suitable primers as a protective coating for above-ground steel structures subjected to atmospheric exposure in industrial areas.

This coating is suitable for use as a topcoat over hot or cold applied coal tar base coatings to provide protection against the deleterious effects of oxidation and ultraviolet radiation in Environmental Zone 1B (exterior, normally dry). It can also be used in heavy industrial environments such as Zones 3A (chemical exposure, acidic), 3B (chemical exposure, neutral), and 3C (chemical exposure, alkaline) where color is not a prime consideration.

(Back to all Standards)

 
   
Advertisements
 
Norton Sandblasting Equipment

 
Paint BidTracker

 
Opta Waterdown, Inc.

 
Modern Safety Techniques

 
base painters

 
Axxiom Manufacturing

 
NLB Corporation

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us