ISO 8993:2010 ISO 8993:2010 Anodized aluminium and aluminium alloys -- Rating system for the evaluation of pitting corrosion -- Chart method

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 02, 2012
Editorial Change:
 
Specifies a chart rating system based on standard charts that provides a means of defining levels of performance of anodic oxide coatings that have been subjected to corrosion tests. This rating system is applicable to pitting corrosion of the basis metal resulting from accelerated tests, exposure to corrosive environments and practical service tests.

(Back to all Standards)

 
   
Advertisements
 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
Norton Sandblasting Equipment
 
Norton Sandblasting Equipment
 
We are a premier stocking distributor for the leading manufacturers of surface preparation equipment, industrial dust collection, vacuums and more.
 

 
US Minerals
 
Blast with the best
 
The most effective blasting media on the market, Black Diamond hits harder and cleans faster.
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
RCG America
 
www.glassOx.com
 
Recycled crushed glass factory direct. Pallet to truckloads. Experience quality. Demand savings. Serving PA, MD, DE, NJ, NY, CT, RI, MA, MI, OH, IN, WV, KY.
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Sauereisen, Inc.
 
Substrate Repair Materials
 

Substrate Repair Materials and Filler Compounds

Sauereisen's full line of underlayments are the ideal substrate repair materials to restore structural integrity prior to the application of SewerGard©
 

 
ARC / A.W. Chesterton Company
 
Corrosion Resistant Coating
 
ARC HT-S incorporates fine graded sizes of reinforcement which contributes to its excellent permeation resistance, resistance to cold-wall delamination, and resistance to thermal-mechanical shock
 

 
Bullard
 
Bullard Made in the USA
 
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us