ISO 11124-1:1993 Preparation of steel substrates before application of paints and related products -- Specifications for metallic blast-cleaning abrasives -- Part 1: General introduction and classification

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Describes a classification and specifies the characteristics which are required for the complete designation of such abrasives. Applies to abrasives supplied in the "new" or unused condition only. Does not apply to abrasives either during or after use.

(Back to all Standards)

 
   
Advertisements
 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
Sauereisen, Inc.
 
Substrate Repair Materials
 

Substrate Repair Materials and Filler Compounds

Sauereisen's full line of underlayments are the ideal substrate repair materials to restore structural integrity prior to the application of SewerGard©
 

 
Jotun Paints Inc.
 
Jotun Jotachar 1709
 
Mesh-free passive fire protection epoxy designed to protect against hydrocarbon pool fire scenarios for up to four hours as defined in the ANSI/UL1709 standard.
 

 
Sky Climber, LLC
 
Solutions in Suspended Access
 
Safely reach workspaces regardless of size or purpose with our full line of Hoists, modular Platforms, and versatile Workcages.
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
SAFE Systems, Inc.
 
Custom blast rooms
by SAFE Systems
 
Don't waste time and money "making do" with a "standard" design. Let us work with you to design and build the system that best fits your requirements.
Call 1-800-634-7278
 

 
Fischer Technology Inc.
 
DUALSCOPE®FMP100 with DataCenter IP
 
Transfer customized inspection plans from PC to FMP100 using step-by-step guidance with prompts and pictures throughout the measurement procedure
 

 
ARC / A.W. Chesterton Company
 
Corrosion Resistant Coating
 
ARC HT-S incorporates fine graded sizes of reinforcement which contributes to its excellent permeation resistance, resistance to cold-wall delamination, and resistance to thermal-mechanical shock
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us