ISO 1249:1974 ISO 1249:1974 Zinc chromate pigments -- Basic zinc potassium chromate pigments and zinc tetrahydroxychromate pigments

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Specifies the requirements and corresponding test methods. The pigments are suitable for use in paints and/or corrosion-inhibiting coatings. Three types of pigments are distinguished. In one typ only a lead content up 2 % maximum is alloqwed. Replaces ISO Recommendation R 1249-1970.

(Back to all Standards)

 
   
Advertisements
 
US Minerals
 
Blast with the best
 
The most effective blasting media on the market, Black Diamond hits harder and cleans faster.
 

 
CHLOR*RID International Inc.
 
SOLUTIONS THAT WORK
 
Companies that invest in corrosion control use CHLOR RID products
  • Soluble salt removal liquid
  • Test kits to verify contamination levels
  • Surface passivation to hold the blast
INFO@CHLOR-RID.COM 800.422.3217
 

 
NLB Corporation
 
NLB Sure Shroud: Greater Protection and Flexibility
 
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-TATOR LABORATORY SERVICES
 
• Coating failure analysis
• Independent testing
• Accelerated weathering testing
• Abrasives Testing
• Oil & Gas Material Qualification
• A2LA Certificate #2455.01
Contact: Rob Leggat
at 412-788-1300 x176
 

 
Blastox/The TDJ Group, Inc.
 
Blastox® - One Step Lead Abatement
 
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!
1(800)-252-7869
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
Fischer Technology Inc.
 
DUALSCOPE®FMP100 with DataCenter IP
 
Transfer customized inspection plans from PC to FMP100 using step-by-step guidance with prompts and pictures throughout the measurement procedure
 

 
Carboline Company
 
New product: Carbozinc® 608 HB
 
Introducing a new high build zinc-rich primer that can save you time and money by eliminating the epoxy intermediate coat!
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us