ISO 787-16:1986 ISO 787-16:1986 General methods of test for pigments and extenders -- Part 16: Determination of relative tinting strength (or equivalent colouring value) and colour on reduction of coloured pigments -- Visual comparison method

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
The complete procedure consists of four parts: determination of the conditions for the preparation of the dispersion of the coloured pigment, and determination of the ratio of the coloured pigment to white pigment; preparation of the dispersion of the coloured pigment under defined conditions on an automatic muller; mixing the dispersions of coloured pigment and white pigment in a known ratio with a white pigment paste

(Back to all Standards)

 
   
Advertisements
 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-Tator Training Course Opportunities
 
• IACET Authorized Continuing Education Unit (CEU) Provider
• Live Basic Coatings Inspection Courses
• Customized/Private Courses
• Online/self-paced curriculums
Contact: Tiffany Kelly at 412-788-1300 x217
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
SSPC: The Society for Protective Coatings
 
http://www.sspc.org/
 
Join SSPC and Enhance
Your Career !
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
US Minerals
 
Blast with the best
 
The most effective blasting media on the market, Black Diamond hits harder and cleans faster.
 

 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
SAFE Systems, Inc.
 
Enduroguard -
The Tough Cable
for a Tough Industry.
 
Reduce maintenance costs and down time, increase job site safety with Enduroguard Cable. Available exclusively from SAFE Systems. UL listed, flexible, abrasion resistant and cut resistant.
 

 
Norton Sandblasting Equipment
 
Norton Sandblasting Equipment
 
We are a premier stocking distributor for the leading manufacturers of surface preparation equipment, industrial dust collection, vacuums and more.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us