ISO 787-11:1981 ISO 787-11:1981 General methods of test for pigments and extenders -- Part 11: Determination of tamped volume and apparent density after tamping

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
The test is carried out by the following procedure: drying of the sample in the oven at (105 2) °C, passing the dried sample through the sieve and transferring it of the graduated measuring cylinder, but so that no air pockets are formed. Weighing of the cylinder and of the sample. Placing of the cylinder in the tamping volumeter and tamping it in steps of approximately 1250 revolutions until the difference between two successive steps of tamping is less than 2 ml. Calculation of results. - Cancels and replaces ISO Recommendation ISO/R 787/11-1970.

(Back to all Standards)

 
   
Advertisements
 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
Fischer Technology Inc.
 
FISCHER Expands Corrosion Product Line
 
Rounding out Fischer’s extensive line of products for measuring protective coatings in the corrosion industry is the new ultrasonic wall thickness gauge UMP series.
 

 
CS Unitec
 
Dust Control Surface Prep Industrial Tools for Steel and Concrete
 
Scarifying • Grinding Scabbling • Descaling Dust collection for safer working conditions. Low-vibration for less worker fatigue. Trelawny™ power tools from CS Unitec. Learn more…
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
ARC / A.W. Chesterton Company
 
Rapid Curing Coating
 
Cures under adverse conditions with maximum adhesion
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
Bullard
 
Bullard Made in the USA
 
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
Sika-Us
 
Sika® Industrial Floor Coatings
 
Click to learn about floor and wall systems relied upon for performance, durability, easy maintenance and aesthetics across the every industry and environment.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us