SSPC-PS 24.00, Latex Painting System for Industrial and Marine Atmospheres, Performance-Based

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: August 01, 1991
Updated On: April 01, 2002
Editorial Change: November 1, 2004
 
This specification covers a painting system for steel surfaces based on multiple coats of air-drying, single-component latex paints having a total dry film thickness of a minimum of six mils (152 micrometers).

A painting system is categorized according to its performance level over blast-cleaned steel, the intended substrate.

The system is suitable for exposure in Environmental Zones 1A (interior, normally dry), 1B (exterior, normally dry), 2A (frequently wet by fresh water), 2B (frequently wet by salt water), 3A (chemical exposure, acidic), 3B (chemical exposure, neutral), 3C (chemical exposure, alkaline) and 3D (chemical exposure, mild solvent).

The system is not intended for immersion service.

(Back to all Standards)

 
   
Advertisements
 
Modern Safety Techniques

 
Paint BidTracker

 
Sauereisen, Inc.

 
Tarps manufacturing, Inc.

 
NLB Corporation

 
Sherwin-Williams

 
CPIA, The Commercial Painting Industry Association

 
EDCO - Equipment Development Co. Inc.

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us