ISO 4628-5:2003 ISO 4628-5:2003 Paints and varnishes -- Evaluation of degradation of paint coatings -- Designation of intensity, quantity and size of common types of defect -- Part 5: Designation of degree of flaking

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 03, 2012
Editorial Change:
 
Provides pictorial standards for rating of flaking.

(Back to all Standards)

 
   
Advertisements
 
HoldTight Solutions Inc.
 
Full Surface Protection for Up to One Year
 
HT 365 is a preservation, single component, anti-corrosive coating, a water displacing agent, a lubricant, and a penetrating fluid. It creates an imperceptible thin-film coating that offers excellent salt contaminant and humidity protection. Contact your HoldTight® representative or visit Holdtight.com for more information.
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-Tator Training Course Opportunities
 
• IACET Authorized Continuing Education Unit (CEU) Provider
• Live Basic Coatings Inspection Courses
• Customized/Private Courses
• Online/self-paced curriculums
Contact: Tiffany Kelly at 412-788-1300 x217
 

 
SAFE Systems, Inc.
 
Portable Dust Collectors for Tough Environments
 
Trailer and skid-mounted models in numerous sizes, powered by electric and/or diesel. Sloped roofs, multiple dust inlets, high static, dampered fans. Lockable power & drive compartments.
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
SABRE Autonomous Solutions
 
Productivity
 
Personnel are free to do other tasks while the ALPHA1 does the “dirty work”.
 

 
Fischer Technology Inc.
 
TSA Coatings on Stainless Steel
 
Fischer’s Phascope PMP10 and ESD20TSA probe are incredibly accurate and easy to use.
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
ARC / A.W. Chesterton Company
 
Rapid Curing Coating
 
Cures under adverse conditions with maximum adhesion
 

 
BASF
 
New resins from BASF will have metals loving water!
 
Excellent corrosion resistance, low VOC, high gloss, thin films www.basf.us/industrialcoatings dpsolutions@basf.com 800-231-7868
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us