ISO 3856-3:1984 ISO 3856-3:1984 Paints and varnishes -- Determination of "soluble" metal content -- Part 3: Determination of barium content -- Flame atomic emission spectrometric method

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
The principle consists in the aspiration of the test solution into a dinitrogen monoxide/acetylene flame. Measurement of the radiation emitted by barium at a wavelength of 553,5 nm.

(Back to all Standards)

 
   
Advertisements
 
Sky Climber, LLC
 
Solutions in Suspended Access
 
Safely reach workspaces regardless of size or purpose with our full line of Hoists, modular Platforms, and versatile Workcages.
 

 
NLB Corporation
 
NLB Sure Shroud: Greater Protection and Flexibility
 
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.
 

 
International Bridge Conference
 
Bridge conference 2018
 
Registration for the 2018 IBC is now open! Join us in June for the biggest and best IBC ever! View the Program, Workshops and Exhibitors by clicking in the banner.
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
Fischer Technology Inc.
 
TSA Coatings on Stainless Steel
 
Fischer’s Phascope PMP10 and ESD20TSA probe are incredibly accurate and easy to use.
 

 
HoldTight Solutions Inc.
 
Full Surface Protection for Up to One Year
 
HT 365 is a preservation, single component, anti-corrosive coating, a water displacing agent, a lubricant, and a penetrating fluid. It creates an imperceptible thin-film coating that offers excellent salt contaminant and humidity protection. Contact your HoldTight® representative or visit Holdtight.com for more information.
 

 
KTA-Tator, Inc. - Corporate Office
 
Instrument Service Department
 
Are you a QP certified contractor? KTA’s Instrument Service Department can help keep you compliant!
Click or call 1-800-KTA-GAGE.
 

 
Blastox/The TDJ Group, Inc.
 
Blastox® - One Step Lead Abatement
 
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!
1(800)-252-7869
 

 
DeFelsko Corporation
 
PosiTector SST Soluble Salt Tester
 
Measures the concentration of soluble salts on metal surfaces. Use with all Bresle patch types including the reusable, adhesive-free PosiPatch.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us