ISO 3856-1:1984 ISO 3856-1:1984 Paints and varnishes -- Determination of "soluble" metal content -- Part 1: Determination of lead content -- Flame atomic absorption spectrometric method and dithizone spectrophotometric method

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
The principle of the AAS method consists in aspiration of the test solution into an acetylen/air flame.

(Back to all Standards)

 
   
Advertisements
 
Sidewinder/Persyst Enterprises, Inc.
 
Sidewinder Model M2
 
Load our Refrigeration Machine Distiller Reclaimer with dirty solvent, press the button, you're done. You will have clean gun wash and cleanup solvents, ready for reuse.
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-TATOR LABORATORY SERVICES
 
• Coating failure analysis
• Independent testing
• Accelerated weathering testing
• Abrasives Testing
• Oil & Gas Material Qualification
• A2LA Certificate #2455.01
Contact: Rob Leggat
at 412-788-1300 x176
 

 
SABRE Autonomous Solutions
 
Repeatability
 
The ALPHA1 provides reliable results consistently allowing you to cost your next job with confidence.
 

 
Norton Sandblasting Equipment
 
Norton Sandblasting Equipment
 
We are a premier stocking distributor for the leading manufacturers of surface preparation equipment, industrial dust collection, vacuums and more.
 

 
RCG America
 
www.glassOx.com
 
Recycled crushed glass factory direct. Pallet to truckloads. Experience quality. Demand savings. Serving PA, MD, DE, NJ, NY, CT, RI, MA, MI, OH, IN, WV, KY.
 

 
SAFE Systems, Inc.
 
Custom blast rooms
by SAFE Systems
 
Don't waste time and money "making do" with a "standard" design. Let us work with you to design and build the system that best fits your requirements.
Call 1-800-634-7278
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
Sauereisen, Inc.
 
Substrate Repair Materials
 

Substrate Repair Materials and Filler Compounds

Sauereisen's full line of underlayments are the ideal substrate repair materials to restore structural integrity prior to the application of SewerGard©
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
SSPC: The Society for Protective Coatings
 
http://www.sspc.org/
 
Join SSPC and Enhance
Your Career !
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us