ISO 2815:2003 ISO 2815:2003 Paints and varnishes -- Buchholz indentation test

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 02, 2012
Editorial Change:
 
Specifies a method for the indentation test under well-defined conditions on a single coating or multicoat system of coating materials or related products.

(Back to all Standards)

 
   
Advertisements
 
CHLOR*RID International Inc.
 
SOLUTIONS THAT WORK
 
Companies that invest in corrosion control use CHLOR RID products
  • Soluble salt removal liquid
  • Test kits to verify contamination levels
  • Surface passivation to hold the blast
INFO@CHLOR-RID.COM 800.422.3217
 

 
HoldTight Solutions Inc.
 
Full Surface Protection for Up to One Year
 
HT 365 is a preservation, single component, anti-corrosive coating, a water displacing agent, a lubricant, and a penetrating fluid. It creates an imperceptible thin-film coating that offers excellent salt contaminant and humidity protection. Contact your HoldTight® representative or visit Holdtight.com for more information.
 

 
DeFelsko Corporation
 
PosiTector SHD Shore Hardness Durometer
 
PosiTector SHD measures the hardness of non-metallic materials. Features a measurement timer, auto ignore mode and internal memory. Shore A or D available.
 

 
US Minerals
 
Blast with the best
 
The most effective blasting media on the market, Black Diamond hits harder and cleans faster.
 

 
Bullard
 
Bullard Made in the USA
 
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-Tator EH&S Services
 
• Ambient & Worker Exposure Air Monitoring
• Safety & Health Program Development
• Lead Paint Assessments
& Specifications
• Health Hazard & Jobsite Safety Assessments
Call 1-800-532-3633
 

 
Carboline Company
 
Carboline launches new website!
 
The completely revamped website, offers quick and easy access to essential product information and is now mobile-friendly.
 

 
Novatek Corporation
 
Dustless Coatings Removal
 
Novatek Corporation, Dustless Coatings Removal Strip, clean and profile all dust free! Comply with new lead standards. Contact today: (866) 563-7800 www.Novatekco.com
 

 
Sika-Us
 
Sika® Industrial Floor Coatings
 
Click to learn about floor and wall systems relied upon for performance, durability, easy maintenance and aesthetics across the every industry and environment.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us