ISO 2813:1994/Cor 1:1997 ISO 2813:1994/Cor 1:1997

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: April 01, 2002
Editorial Change:
 
Contains some amendments intended to improve the repeatability and reproducibility of specular-gloss measurements. Contains some amendments intended to improve the repeatability and reproducibility of specular-gloss measurements. Contains some amendments intended to improve the repeatability and reproducibility of specular-gloss measurements.

(Back to all Standards)

 
   
Advertisements
 
US Minerals
 
Blast with the best
 
The most effective blasting media on the market, Black Diamond hits harder and cleans faster.
 

 
Tarps manufacturing, Inc.
 
QUALITY MADE IN AMERICA —Available near you!
 
CLICK to get a behind-the-scenes look at how Tarps Manufacturing makes the highest-quality tarps right here in the USA — available nationwide.
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-TATOR LABORATORY SERVICES
 
• Coating failure analysis
• Independent testing
• Accelerated weathering testing
• Abrasives Testing
• Oil & Gas Material Qualification
• A2LA Certificate #2455.01
Contact: Rob Leggat
at 412-788-1300 x176
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
Sky Climber, LLC
 
Solutions in Suspended Access
 
Safely reach workspaces regardless of size or purpose with our full line of Hoists, modular Platforms, and versatile Workcages.
 

 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
SSPC: The Society for Protective Coatings
 
http://www.sspc.org/
 
Join SSPC and Enhance
Your Career !
 

 
ARC / A.W. Chesterton Company
 
Mils Ahead of the Competition
 
Excellent chemical resistance where erosive particulates and thermal cycling conditions may be present.
 

 
SABRE Autonomous Solutions
 
Repeatability
 
The ALPHA1 provides reliable results consistently allowing you to cost your next job with confidence.
 

 
NLB Corporation
 
NLB Sure Shroud: Greater Protection and Flexibility
 
NLB’s Sure Shroud’s lighter weight and flexibility reduces operator fatigue and offers unmatched protection against high pressure hose ruptures. 10k to 40k psi rated.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us