ISO 2812-1:2007 ISO 2812-1:2007 Paints and varnishes -- Determination of resistance to liquids -- Part 1: General methods

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 02, 2012
Editorial Change:
 
The principle is exposing a coated test panel to a liquid by one of three specified methods (the immersion method using a single-phase liquid or a two-phase liquid, a method with the use of an absorbent medium, and the spotting method) and evaluating the effects of exposure by criteria agreed in advance between the interested parties

(Back to all Standards)

 
   
Advertisements
 
Graco Inc.
 
Graco EcoQuip 2: Experience the Difference
 
While others claim their equipment is the same, none of them compare to Graco’s EcoQuip 2™ Vapor Abrasive® blasting line. Visit graco.com/ecoquip to learn more.
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
Blastox/The TDJ Group, Inc.
 
Blastox® - One Step Lead Abatement
 
Sandblast additive delivered to jobsite pre-blended to eliminate hazardous abrasive wastes. Why mix, meter or apply at the job-site? Blast with ease and
Let your painters paint!
1(800)-252-7869
 

 
Modern Safety Techniques
 
Modern Safety Techniques
 
With our unique LTCat, we can help to provide clean, safe breathing air to your workers. Take a look at our Breathing Air Systems, we supply at least twice as much charcoal as our competitors! Modern
 

 
KTA-Tator, Inc. - Corporate Office
 
KTA-Tator EH&S Services
 
• Ambient & Worker Exposure Air Monitoring
• Safety & Health Program Development
• Lead Paint Assessments
& Specifications
• Health Hazard & Jobsite Safety Assessments
Call 1-800-532-3633
 

 
SSPC: The Society for Protective Coatings
 
http://www.sspc.org/
 
Join SSPC and Enhance
Your Career !
 

 
Fischer Technology Inc.
 
TSA Coatings on Stainless Steel
 
Fischer’s Phascope PMP10 and ESD20TSA probe are incredibly accurate and easy to use.
 

 
Bullard
 
Bullard Made in the USA
 
 

 
Novatek Corporation
 
Dustless Coatings Removal
 
Novatek Corporation, Dustless Coatings Removal Strip, clean and profile all dust free! Comply with new lead standards. Contact today: (866) 563-7800 www.Novatekco.com
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us