ISO 2431:2011 ISO 2431:2011

All Standards | ISO Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date:
Updated On: August 02, 2012
Editorial Change:
 
Replaces figure 1 by a figure, in which the mouth of the jet is 0,1 mm below the cup body in order to minimize eddy-current effects

(Back to all Standards)

 
   
Advertisements
 
ABKaelin, LLC
 
ABKAELIN EH&S SERVICES
 
Programs/Training/Monitoring for Silica, Lead, Noise, Beryllium, Hexavalent Chromium, Cadmium, Hazardous Waste*PM10 & TSP-Lead Ambient Air Monitoring*SSPC C3/C5
 

 
SABRE Autonomous Solutions
 
Productivity
 
Personnel are free to do other tasks while the ALPHA1 does the “dirty work”.
 

 
SSPC: The Society for Protective Coatings
 
http://www.sspc.org/
 
Join SSPC and Enhance
Your Career !
 

 
Industrial Vacuum Equipment Corp.
 
Hurricane Vacuums
& Dust Collectors
 
Vacuum and dust collector hose, filters and related accessories.
IndustrialVacuum.com
 

 
Sky Climber, LLC
 
Solutions in Suspended Access
 
Safely reach workspaces regardless of size or purpose with our full line of Hoists, modular Platforms, and versatile Workcages.
 

 
Mitsubishi Gas Chemical America
 
Performance Amine 1,3-BAC
 
A highly reactive cycloaliphatic diamine offering superior performance. Reasonable cost and curing efficacy makes it suitable for all types of epoxy resin applications.
 

 
Carboline Company
 
Carboline launches new website!
 
The completely revamped website, offers quick and easy access to essential product information and is now mobile-friendly.
 

 
Absolute Equipment/Grand Rental Station
 
TIER 4 EQUIPMENT
 
We have Tier 4 Equipment including Air Compressors & Generators for Sale & Rent! Your job may now require Tier-4. www.absoluteequip.com or Call 412-931-6655.
 

 
 

 
DeFelsko Corporation
 
PosiTector SHD Shore Hardness Durometer
 
PosiTector SHD measures the hardness of non-metallic materials. Features a measurement timer, auto ignore mode and internal memory. Shore A or D available.
 

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

Durability + Design PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy (Updated 5/24/2018)   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us