SSPC-PS 10.02, Cold-Applied Coal Tar Mastic Painting System

All Standards | SSPC Standards
Search Standards


Click to Purchase and Download this Standard or Test Method

Revision Date: November 01, 1982
Updated On: April 01, 2002
Editorial Change: November 1, 2004
 
This specification covers a cold-applied coal tar painting system for underground and underwater steel structures,consisting of two cold-applied coats.

This system is suitable for use on parts or structures exposed in Environmental Zones 2C (fresh water immersion), 3B (chemical exposure, neutral), and 3C (chemical exposure, alkaline). It has fairly good abrasion resistance and is suitable for underground use. It must be used with discretion for immersion in corrosive chemicals since the coating is dissolved by some organic solvents and attacked by oxidizing solutions.

The coal tar mastic must be topcoated with coal tar emulsion when exposed to sunlight to prevent checking and alligatoring.

(Back to all Standards)

 
   
Advertisements
 
NLB Corporation

 
Norton Sandblasting Equipment

 
Tarps manufacturing, Inc.

 
Thomas Industrial Coatings, Inc.

 
Paint BidTracker

 
Modern Safety Techniques

 
base painters

 
Opta Waterdown, Inc.

 
Sauereisen, Inc.

 
Axxiom Manufacturing

 
 
 

Technology Publishing Co., 1501 Reedsdale Street, Suite 2008, Pittsburgh, PA 15233

TEL 1-412-431-8300  • FAX  1-412-431-5428  •  EMAIL webmaster@paintsquare.com


The Technology Publishing Network

PaintSquare the Journal of Protective Coatings & Linings Paint BidTracker

 
EXPLORE:      JPCL   |   PaintSquare News   |   Interact   |   Buying Guides   |   Webinars   |   Resources   |   Classifieds
REGISTER AND SUBSCRIBE:      Free PaintSquare Registration   |   Subscribe to JPCL   |   Subscribe to PaintSquare News
MORE:      About PaintSquare.com   |   Privacy Policy   |   Terms & Conditions   |   Support   |   Site Map   |   Search   |   Contact Us